26
|
Simpson JR, Roslyak O, Duque JG, Hároz EH, Crochet JJ, Telg H, Piryatinski A, Walker ARH, Doorn SK. Resonance Raman signature of intertube excitons in compositionally-defined carbon nanotube bundles. Nat Commun 2018; 9:637. [PMID: 29434198 PMCID: PMC5809379 DOI: 10.1038/s41467-018-03057-7] [Citation(s) in RCA: 10] [Impact Index Per Article: 1.7] [Reference Citation Analysis] [Abstract] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 09/06/2017] [Accepted: 01/17/2018] [Indexed: 11/23/2022] Open
Abstract
Electronic interactions in low-dimensional nanomaterial heterostructures can lead to novel optical responses arising from exciton delocalization over the constituent materials. Similar phenomena have been suggested to arise between closely interacting semiconducting carbon nanotubes of identical structure. Such behavior in carbon nanotubes has potential to generate new exciton physics, impact exciton transport mechanisms in nanotube networks, and place nanotubes as one-dimensional models for such behaviors in systems of higher dimensionality. Here we use resonance Raman spectroscopy to probe intertube interactions in (6,5) chirality-enriched bundles. Raman excitation profiles for the radial breathing mode and G-mode display a previously unobserved sharp resonance feature. We show the feature is evidence for creation of intertube excitons and is identified as a Fano resonance arising from the interaction between intratube and intertube excitons. The universality of the model suggests that similar Raman excitation profile features may be observed for interlayer exciton resonances in 2D multilayered systems. Bundles of single-wall carbon nanotubes with enriched chirality can be used as model systems for exploring exciton physics in low-dimensional nanostructures. Here, the authors use resonant Raman spectroscopy to probe intertube interactions in bundles of (6,5)-enriched carbon nanotubes, and observe a Fano resonance arising from coupling between intertube and intratube excitons.
Collapse
|
27
|
He X, Gifford BJ, Hartmann NF, Ihly R, Ma X, Kilina SV, Luo Y, Shayan K, Strauf S, Blackburn JL, Tretiak S, Doorn SK, Htoon H. Low-Temperature Single Carbon Nanotube Spectroscopy of sp 3 Quantum Defects. ACS NANO 2017; 11:10785-10796. [PMID: 28958146 DOI: 10.1021/acsnano.7b03022] [Citation(s) in RCA: 59] [Impact Index Per Article: 8.4] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 05/27/2023]
Abstract
Aiming to unravel the relationship between chemical configuration and electronic structure of sp3 defects of aryl-functionalized (6,5) single-walled carbon nanotubes (SWCNTs), we perform low-temperature single nanotube photoluminescence (PL) spectroscopy studies and correlate our observations with quantum chemistry simulations. We observe sharp emission peaks from individual defect sites that are spread over an extremely broad, 1000-1350 nm, spectral range. Our simulations allow us to attribute this spectral diversity to the occurrence of six chemically and energetically distinct defect states resulting from topological variation in the chemical binding configuration of the monovalent aryl groups. Both PL emission efficiency and spectral line width of the defect states are strongly influenced by the local dielectric environment. Wrapping the SWCNT with a polyfluorene polymer provides the best isolation from the environment and yields the brightest emission with near-resolution limited spectral line width of 270 μeV, as well as spectrally resolved emission wings associated with localized acoustic phonons. Pump-dependent studies further revealed that the defect states are capable of emitting single, sharp, isolated PL peaks over 3 orders of magnitude increase in pump power, a key characteristic of two-level systems and an important prerequisite for single-photon emission with high purity. These findings point to the tremendous potential of sp3 defects in development of room temperature quantum light sources capable of operating at telecommunication wavelengths as the emission of the defect states can readily be extended to this range via use of larger diameter SWCNTs.
Collapse
|
28
|
Ma X, Hartmann NF, Velizhanin KA, Baldwin JKS, Adamska L, Tretiak S, Doorn SK, Htoon H. Multi-exciton emission from solitary dopant states of carbon nanotubes. NANOSCALE 2017; 9:16143-16148. [PMID: 29053165 DOI: 10.1039/c7nr06661a] [Citation(s) in RCA: 3] [Impact Index Per Article: 0.4] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/07/2023]
Abstract
By separating the photons from slow and fast decays of single and multi-exciton states in a time gated 2nd order photon correlation experiment, we show that solitary oxygen dopant states of single-walled carbon nanotubes (SWCNTs) allow emission of photon pairs with efficiencies as high as 44% of single exciton emission. Our pump dependent time resolved photoluminescence (PL) studies further reveal diffusion-limited exciton-exciton annihilation as the key process that limits the emission of multi-excitons at high pump fluences. We further postulate that creation of additional permanent exciton quenching sites occurring under intense laser irradiation leads to permanent PL quenching. With this work, we bring out multi-excitonic processes of solitary dopant states as a new area to be explored for potential applications in lasing and entangled photon generation.
Collapse
|
29
|
Ma X, James AR, Hartmann NF, Baldwin JK, Dominguez J, Sinclair MB, Luk TS, Wolf O, Liu S, Doorn SK, Htoon H, Brener I. Solitary Oxygen Dopant Emission from Carbon Nanotubes Modified by Dielectric Metasurfaces. ACS NANO 2017; 11:6431-6439. [PMID: 28535349 DOI: 10.1021/acsnano.7b02951] [Citation(s) in RCA: 3] [Impact Index Per Article: 0.4] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/07/2023]
Abstract
All-dielectric metasurfaces made from arrays of high index nanoresonators supporting strong magnetic dipole modes have emerged as a low-loss alternative to plasmonic metasurfaces. Here we use oxygen-doped single-walled carbon nanotubes (SWCNTs) as quantum emitters and couple them to silicon metasurfaces to study effects of the magnetic dipole modes of the constituent nanoresonators on the photoluminescence (PL) of individual SWCNTs. We find that when in resonance, the magnetic mode of the silicon nanoresonators can lead to a moderate average PL enhancement of 0.8-4.0 of the SWCNTs, accompanied by an average increase in the radiative decay rate by a factor of 1.5-3.0. More interestingly, single dopant polarization experiments show an anomalous photoluminescence polarization rotation by coupling individual SWCNTs to silicon nanoresonators. Numerical simulations indicate that this is caused by modification of near-field polarization distribution at certain areas in the proximity of the silicon nanoresonators at the excitation wavelength, thus presenting an approach to control emission polarization. These findings indicate silicon nanoresonators as potential building blocks of quantum photonic circuits capable of manipulating PL intensity and polarization of single photon sources.
Collapse
|
30
|
Ma X, Cambré S, Wenseleers W, Doorn SK, Htoon H. Quasiphase Transition in a Single File of Water Molecules Encapsulated in (6,5) Carbon Nanotubes Observed by Temperature-Dependent Photoluminescence Spectroscopy. PHYSICAL REVIEW LETTERS 2017; 118:027402. [PMID: 28128601 DOI: 10.1103/physrevlett.118.027402] [Citation(s) in RCA: 16] [Impact Index Per Article: 2.3] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Received: 05/01/2016] [Indexed: 05/14/2023]
Abstract
Molecules confined inside single-walled carbon nanotubes (SWCNTs) behave quite differently from their bulk analogues. In this Letter we present temperature-dependent (4.2 K up to room temperature) photoluminescence (PL) spectra of water-filled and empty single-chirality (6,5) SWCNTs. Superimposed on a linear temperature-dependent PL spectral shift of the empty SWCNTs, an additional stepwise PL spectral shift of the water-filled SWCNTs is observed at ∼150 K. With the empty SWCNTs serving as an ideal reference system, we assign this shift to temperature-induced changes occurring in the single-file chain of water molecules encapsulated in the tubes. Our molecular dynamics simulations further support the occurrence of a quasiphase transition of the orientational order of the water dipoles in the single-file chain.
Collapse
|
31
|
Mallajosyula AT, Nie W, Gupta G, Blackburn JL, Doorn SK, Mohite AD. Critical Role of the Sorting Polymer in Carbon Nanotube-Based Minority Carrier Devices. ACS NANO 2016; 10:10808-10815. [PMID: 27966903 DOI: 10.1021/acsnano.6b04885] [Citation(s) in RCA: 2] [Impact Index Per Article: 0.3] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/06/2023]
Abstract
A prerequisite for carbon nanotube-based optoelectronic devices is the ability to sort them into a pure semiconductor phase. One of the most common sorting routes is enabled through using specific wrapping polymers. Here we show that subtle changes in the polymer structure can have a dramatic influence on the figures of merit of a carbon nanotube-based photovoltaic device. By comparing two commonly used polyfluorenes (PFO and PFO-BPy) for wrapping (7,5) and (6,5) chirality SWCNTs, we demonstrate that they have contrasting effects on the device efficiency. We attribute this to the differences in their ability to efficiently transfer charge. Although PFO may act as an efficient interfacial layer at the anode, PFO-BPy, having the additional pyridine side groups, forms a high resistance layer degrading the device efficiency. By comparing PFO|C60 and C60-only devices, we found that presence of a PFO layer at low optical densities resulted in the increase of all three solar cell parameters, giving nearly an order of magnitude higher efficiency over that of C60-only devices. In addition, with a relatively higher contribution to photocurrent from the PFO-C60 interface, an open circuit voltage of 0.55 V was obtained for PFO-(7,5)-C60 devices. On the other hand, PFO-BPy does not affect the open circuit voltage but drastically reduces the short circuit current density. These results indicate that the charge transport properties and energy levels of the sorting polymers have to be taken into account to fully understand their effect on carbon nanotube-based solar cells.
Collapse
|
32
|
Hartmann NF, Pramanik R, Dowgiallo AM, Ihly R, Blackburn JL, Doorn SK. Photoluminescence Imaging of Polyfluorene Surface Structures on Semiconducting Carbon Nanotubes: Implications for Thin Film Exciton Transport. ACS NANO 2016; 10:11449-11458. [PMID: 27936574 DOI: 10.1021/acsnano.6b07168] [Citation(s) in RCA: 2] [Impact Index Per Article: 0.3] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/06/2023]
Abstract
Single-walled carbon nanotubes (SWCNTs) have potential to act as light-harvesting elements in thin film photovoltaic devices, but performance is in part limited by the efficiency of exciton diffusion processes within the films. Factors contributing to exciton transport can include film morphology encompassing nanotube orientation, connectivity, and interaction geometry. Such factors are often defined by nanotube surface structures that are not yet well understood. Here, we present the results of a combined pump-probe and photoluminescence imaging study of polyfluorene (PFO)-wrapped (6,5) and (7,5) SWCNTs that provide additional insight into the role played by polymer structures in defining exciton transport. Pump-probe measurements suggest exciton transport occurs over larger length scales in films composed of PFO-wrapped (7,5) SWCNTs, compared to those prepared from PFO-bpy-wrapped (6,5) SWCNTs. To explore the role the difference in polymer structure may play as a possible origin of differing transport behaviors, we performed a photoluminescence imaging study of individual polymer-wrapped (6,5) and (7,5) SWCNTs. The PFO-bpy-wrapped (6,5) SWCNTs showed more uniform intensity distributions along their lengths, in contrast to the PFO-wrapped (7,5) SWCNTs, which showed irregular, discontinuous intensity distributions. These differences likely originate from differences in surface coverage and suggest the PFO wrapping on (7,5) nanotubes produces a more open surface structure than is available with the PFO-bpy wrapping of (6,5) nanotubes. The open structure likely leads to improved intertube coupling that enhances exciton transport within the (7,5) films, consistent with the results of our pump-probe measurements.
Collapse
|
33
|
Hartmann NF, Velizhanin KA, Haroz EH, Kim M, Ma X, Wang Y, Htoon H, Doorn SK. Photoluminescence Dynamics of Aryl sp(3) Defect States in Single-Walled Carbon Nanotubes. ACS NANO 2016; 10:8355-65. [PMID: 27529740 DOI: 10.1021/acsnano.6b02986] [Citation(s) in RCA: 55] [Impact Index Per Article: 6.9] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 05/18/2023]
Abstract
Photoluminescent defect states introduced by sp(3) functionalization of semiconducting carbon nanotubes are rapidly emerging as important routes for boosting emission quantum yields and introducing new functionality. Knowledge of the relaxation dynamics of these states is required for understanding how functionalizing agents (molecular dopants) may be designed to access specific behaviors. We measure photoluminescence (PL) decay dynamics of sp(3) defect states introduced by aryl functionalization of the carbon nanotube surface. Results are given for five different nanotube chiralities, each doped with a range of aryl functionality. We find that the PL decays of these sp(3) defect states are biexponential, with both components relaxing on time scales of ∼100 ps. Exciton trapping at defects is found to increases PL lifetimes by a factor of 5-10, in comparison to those for the free exciton. A significant chirality dependence is observed in the decay times, ranging from 77 ps for (7,5) nanotubes to >600 ps for (5,4) structures. The strong correlation of time constants with emission energy indicates relaxation occurs via multiphonon decay processes, with close agreement to theoretical expectations. Variation of the aryl dopant further modulates decay times by 10-15%. The aryl defects also affect PL lifetimes of the free E11 exciton. Shortening of the E11 bright state lifetime as defect density increases provides further confirmation that defects act as exciton traps. A similar shortening of the E11 dark exciton lifetime is found as defect density increases, providing strong experimental evidence that dark excitons are also trapped at such defect sites.
Collapse
|
34
|
He X, Gao W, Xie L, Li B, Zhang Q, Lei S, Robinson JM, Hároz EH, Doorn SK, Wang W, Vajtai R, Ajayan PM, Adams WW, Hauge RH, Kono J. Wafer-scale monodomain films of spontaneously aligned single-walled carbon nanotubes. NATURE NANOTECHNOLOGY 2016; 11:633-8. [PMID: 27043199 DOI: 10.1038/nnano.2016.44] [Citation(s) in RCA: 132] [Impact Index Per Article: 16.5] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Received: 07/25/2015] [Accepted: 02/19/2016] [Indexed: 05/02/2023]
Abstract
The one-dimensional character of electrons, phonons and excitons in individual single-walled carbon nanotubes leads to extremely anisotropic electronic, thermal and optical properties. However, despite significant efforts to develop ways to produce large-scale architectures of aligned nanotubes, macroscopic manifestations of such properties remain limited. Here, we show that large (>cm(2)) monodomain films of aligned single-walled carbon nanotubes can be prepared using slow vacuum filtration. The produced films are globally aligned within ±1.5° (a nematic order parameter of ∼1) and are highly packed, containing 1 × 10(6) nanotubes in a cross-sectional area of 1 μm(2). The method works for nanotubes synthesized by various methods, and film thickness is controllable from a few nanometres to ∼100 nm. We use the approach to create ideal polarizers in the terahertz frequency range and, by combining the method with recently developed sorting techniques, highly aligned and chirality-enriched nanotube thin-film devices. Semiconductor-enriched devices exhibit polarized light emission and polarization-dependent photocurrent, as well as anisotropic conductivities and transistor action with high on/off ratios.
Collapse
|
35
|
Hartmann NF, Yalcin SE, Adamska L, Hároz EH, Ma X, Tretiak S, Htoon H, Doorn SK. Photoluminescence imaging of solitary dopant sites in covalently doped single-wall carbon nanotubes. NANOSCALE 2015; 7:20521-20530. [PMID: 26586162 DOI: 10.1039/c5nr06343d] [Citation(s) in RCA: 34] [Impact Index Per Article: 3.8] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 05/29/2023]
Abstract
Covalent dopants in semiconducting single wall carbon nanotubes (SWCNTs) are becoming important as routes for introducing new photoluminescent emitting states with potential for enhanced quantum yields, new functionality, and as species capable of near-IR room-temperature single photon emission. The origin and behavior of the dopant-induced emission is thus important to understand as a key requirement for successful room-T photonics and optoelectronics applications. Here, we use direct correlated two-color photoluminescence imaging to probe how the interplay between the SWCNT bright E(11) exciton and solitary dopant sites yields the dopant-induced emission for three different dopant species: oxygen, 4-methoxybenzene, and 4-bromobenzene. We introduce a route to control dopant functionalization to a low level as a means for introducing spatially well-separated solitary dopant sites. Resolution of emission from solitary dopant sites and correlation to their impact on E(11) emission allows confirmation of dopants as trapping sites for localization of E(11) excitons following their diffusive transport to the dopant site. Imaging of the dopant emission also reveals photoluminescence intermittency (blinking), with blinking dynamics being dependent on the specific dopant. Density functional theory calculations were performed to evaluate the stability of dopants and delineate the possible mechanisms of blinking. Theoretical modeling suggests that the trapping of free charges in the potential well created by permanent dipoles introduced by dopant atoms/groups is likely responsible for the blinking, with the strongest effects being predicted and observed for oxygen-doped SWCNTs.
Collapse
|
36
|
Adamska L, Nazin GV, Doorn SK, Tretiak S. Self-Trapping of Charge Carriers in Semiconducting Carbon Nanotubes: Structural Analysis. J Phys Chem Lett 2015; 6:3873-3879. [PMID: 26722885 DOI: 10.1021/acs.jpclett.5b01729] [Citation(s) in RCA: 5] [Impact Index Per Article: 0.6] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 06/05/2023]
Abstract
The spatial extent of charged electronic states in semiconducting carbon nanotubes with indices (6,5) and (7,6) was evaluated using density functional theory. It was observed that electrons and holes self-trap along the nanotube axis on length scales of about 4 and 8 nm, respectively, which localize cations and anions on comparable length scales. Self-trapping is accompanied by local structural distortions showing periodic bond-length alternation. The average lengthening (shortening) of the bonds for anions (cations) is expected to shift the G-mode frequency to lower (higher) values. The smaller-diameter nanotube has reduced structural relaxation due to higher carbon-carbon bond strain. The reorganization energy due to charge-induced deformations in both nanotubes is found to be in the 30-60 meV range. Our results represent the first theoretical simulation of self-trapping of charge carriers in semiconducting nanotubes, and agree with available experimental data.
Collapse
|
37
|
Ma X, Hartmann NF, Baldwin JKS, Doorn SK, Htoon H. Room-temperature single-photon generation from solitary dopants of carbon nanotubes. NATURE NANOTECHNOLOGY 2015; 10:671-5. [PMID: 26167766 DOI: 10.1038/nnano.2015.136] [Citation(s) in RCA: 116] [Impact Index Per Article: 12.9] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Received: 01/28/2015] [Accepted: 06/02/2015] [Indexed: 05/23/2023]
Abstract
On-demand single-photon sources capable of operating at room temperature and the telecom wavelength range of 1,300-1,500 nm hold the key to the realization of novel technologies that span from sub-diffraction imaging to quantum key distribution and photonic quantum information processing. Here, we show that incorporation of undoped (6,5) single-walled carbon nanotubes into a SiO2 matrix can lead to the creation of solitary oxygen dopant states capable of fluctuation-free, room-temperature single-photon emission in the 1,100-1,300 nm wavelength range. We investigated the effects of temperature on photoluminescence emission efficiencies, fluctuations and decay dynamics of the dopant states and determined the conditions most suitable for the observation of single-photon emission. This emission can in principle be extended to 1,500 nm by doping of smaller-bandgap single-walled carbon nanotubes. This easy tunability presents a distinct advantage over existing defect centre single-photon emitters (for example, diamond defect centres). Our SiO2-encapsulated sample also presents exciting opportunities to apply Si/SiO2-based micro/nano-device fabrication techniques in the development of electrically driven single-photon sources and integration of these sources into quantum photonic devices and networks.
Collapse
|
38
|
Ma X, Roslyak O, Duque JG, Pang X, Doorn SK, Piryatinski A, Dunlap DH, Htoon H. Influences of Exciton Diffusion and Exciton-Exciton Annihilation on Photon Emission Statistics of Carbon Nanotubes. PHYSICAL REVIEW LETTERS 2015; 115:017401. [PMID: 26182119 DOI: 10.1103/physrevlett.115.017401] [Citation(s) in RCA: 10] [Impact Index Per Article: 1.1] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Received: 01/23/2014] [Indexed: 06/04/2023]
Abstract
Pump-dependent photoluminescence imaging and second-order photon correlation studies have been performed on individual single-walled carbon nanotubes (SWCNTs) at room temperature. These studies enable the extraction of both the exciton diffusion constant and the Auger recombination coefficient. A linear correlation between these parameters is attributed to the effect of environmental disorder in setting the exciton mean free path and capture-limited Auger recombination at this length scale. A suppression of photon antibunching is attributed to the creation of multiple spatially nonoverlapping excitons in SWCNTs, whose diffusion length is shorter than the laser spot size. We conclude that complete antibunching at room temperature requires an enhancement of the exciton-exciton annihilation rate that may become realizable in SWCNTs allowing for strong exciton localization.
Collapse
|
39
|
Fagan JA, Hároz EH, Ihly R, Gui H, Blackburn JL, Simpson JR, Lam S, Hight Walker AR, Doorn SK, Zheng M. Isolation of >1 nm Diameter Single-Wall Carbon Nanotube Species Using Aqueous Two-Phase Extraction. ACS NANO 2015; 9:5377-90. [PMID: 25871430 DOI: 10.1021/acsnano.5b01123] [Citation(s) in RCA: 73] [Impact Index Per Article: 8.1] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 05/12/2023]
Abstract
In this contribution we demonstrate the effective separation of single-wall carbon nanotube (SWCNT) species with diameters larger than 1 nm through multistage aqueous two-phase extraction (ATPE), including isolation at the near-monochiral species level up to at least the diameter range of SWCNTs synthesized by electric arc synthesis (1.3-1.6 nm). We also demonstrate that refined species are readily obtained from both the metallic and semiconducting subpopulations of SWCNTs and that this methodology is effective for multiple SWCNT raw materials. Using these data, we report an empirical function for the necessary surfactant concentrations in the ATPE method for separating different SWCNTs into either the lower or upper phase as a function of SWCNT diameter. This empirical correlation enables predictive separation design and identifies a subset of SWCNTs that behave unusually as compared to other species. These results not only dramatically increase the range of SWCNT diameters to which species selective separation can be achieved but also demonstrate that aqueous two-phase separations can be designed across experimentally accessible ranges of surfactant concentrations to controllably separate SWCNT populations of very small (∼0.62 nm) to very large diameters (>1.7 nm). Together, the results reported here indicate that total separation of all SWCNT species is likely feasible by the ATPE method, especially given future development of multistage automated extraction techniques.
Collapse
|
40
|
Abstract
Polyclic aromatic hydrocarbons also called Graphene Molecules (GMs), with chemical composition C132H36(COOH)2 were synthesized in situ on the surface of transparent nanocrystalline indium tin oxide (nc-ITO) electrodes and their electronic structure was studied electrochemically and spectro-electrochemically. Variations in the potential applied onto the nc-ITO/GM electrodes induce only small changes in the observed current, but they produce dramatic changes in the absorption of the GMs, which are associated with their oxidation and reduction. Analysis of the absorption changes using a modified Nernst equation is used to determine standard potentials associated with the individual charge transfer processes. For the GMs prepared here, these were found to be E1,ox(0) = 0.77 ± 0.01 V and E2,ox(0) = 1.24 ± 0.02 V vs NHE for the first and second oxidation and E1,red(0) = -1.50 ± 0.04 V for the first reduction. The charge transfer processes are found to be nonideal. The nonideality factors associated with the oxidation and reduction processes are attributed to strong interactions between the GM redox centers. Under the conditions of potential cycling, GMs show rapid (seconds) color change with high contrast and stability. An electrochromic application is demonstrated wherein the GMs are used as the optically active component.
Collapse
|
41
|
Yalcin SE, Galande C, Kappera R, Yamaguchi H, Martinez U, Velizhanin KA, Doorn SK, Dattelbaum AM, Chhowalla M, Ajayan PM, Gupta G, Mohite AD. Direct imaging of charge transport in progressively reduced graphene oxide using electrostatic force microscopy. ACS NANO 2015; 9:2981-2988. [PMID: 25668323 DOI: 10.1021/nn507150q] [Citation(s) in RCA: 3] [Impact Index Per Article: 0.3] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/04/2023]
Abstract
Graphene oxide (GO) has emerged as a multifunctional material that can be synthesized in bulk quantities and can be solution processed to form large-area atomic layered photoactive, flexible thin films for optoelectronic devices. This is largely due to the potential ability to tune electrical and optical properties of GO using functional groups. For the successful application of GO, it is key to understand the evolution of its optoelectronic properties as the GO undergoes a phase transition from its insulating and optically active state to the electrically conducting state with progressive reduction. In this paper, we use a combination of electrostatic force microscopy (EFM) and optical spectroscopy to monitor the emergence of the optoelectronic properties of GO with progressive reduction. EFM measurements enable, for the first time, direct visualization of charge propagation along the conducting pathways that emerge on progressively reduced graphene oxide (rGO) and demonstrate that with the increasing degree of reduction, injected charges can rapidly migrate over a distance of several micrometers, irrespective of their polarities. Direct imaging reveals the presence of an insurmountable potential barrier between reduced GO (rGO) and GO, which plays the decisive role in the charge transport. We complement charge imaging with theoretical modeling using quantum chemistry calculations that further demonstrate that the role of barrier in regulating the charge transport. Furthermore, by correlating the EFM measurements with photoluminescence imaging and electrical conductivity studies, we identify a bifunctional state in GO, where the optical properties are preserved along with good electrical conductivity, providing design principles for the development of GO-based, low-cost, thin-film optoelectronic applications.
Collapse
|
42
|
Liu J, Adamska L, Doorn SK, Tretiak S. Singlet and triplet excitons and charge polarons in cycloparaphenylenes: a density functional theory study. Phys Chem Chem Phys 2015; 17:14613-22. [DOI: 10.1039/c5cp01782c] [Citation(s) in RCA: 18] [Impact Index Per Article: 2.0] [Reference Citation Analysis] [Abstract] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 12/14/2022]
Abstract
Upon excitation, electron–phonon coupling leads to spatial localization of the electronic wavefunction and distortion of molecular geometry.
Collapse
|
43
|
Ignatova T, Blades M, Duque JG, Doorn SK, Biaggio I, Rotkin SV. Formation and dynamics of "waterproof" photoluminescent complexes of rare earth ions in crowded environment. Phys Chem Chem Phys 2014; 16:26715-21. [PMID: 25379879 DOI: 10.1039/c4cp04342a] [Citation(s) in RCA: 1] [Impact Index Per Article: 0.1] [Reference Citation Analysis] [Abstract] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 01/20/2023]
Abstract
Understanding behavior of rare-earth ions (REI) in crowded environments is crucial for several nano- and bio-technological applications. Evolution of REI photoluminescence (PL) in small compartments inside a silica hydrogel, mimic to a soft matter bio-environment, has been studied and explained within a solvation model. The model uncovered the origin of high PL efficiency to be the formation of REI complexes, surrounded by bile salt (DOC) molecules. Comparative study of these REI-DOC complexes in bulk water solution and those enclosed inside the hydrogel revealed a strong correlation between an up to 5×-longer lifetime of REIs and appearance of the DOC ordered phase, further confirmed by dynamics of REI solvation shells, REI diffusion experiments and morphological characterization of microstructure of the hydrogel.
Collapse
|
44
|
Ji Z, Wu R, Adamska L, Velizhanin KA, Doorn SK, Sykora M. In situ synthesis of graphene molecules on TiO2: application in sensitized solar cells. ACS APPLIED MATERIALS & INTERFACES 2014; 6:20473-20478. [PMID: 25322280 DOI: 10.1021/am506047f] [Citation(s) in RCA: 5] [Impact Index Per Article: 0.5] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/04/2023]
Abstract
We present a method for preparation of graphene molecules (GMs), whereby a polyphenylene precursor functionalized with surface anchoring groups, preadsorbed on surface of TiO2, is oxidatively dehydrogenated in situ via a Scholl reaction. The reaction, performed at ambient conditions, yields surface adsorbed GMs structurally and electronically equivalent to those synthesized in solution. The new synthetic approach reduces the challenges associated with the tendency of GMs to aggregate and provides a convenient path for integration of GMs into optoelectronic applications. The surface synthesized GMs can be effectively reduced or oxidized via an interfacial charge transfer and can also function as sensitizers for metal oxides in light harvesting applications. Sensitized solar cells (SSCs) prepared from mesoscopic TiO2/GM films and an iodide-based liquid electrolyte show photocurrents of ∼2.5 mA/cm2, an open circuit voltage of ∼0.55 V and fill factor of ∼0.65 under AM 1.5 illumination. The observed power conversion efficiency of η=0.87% is the highest reported efficiency for the GM sensitized solar cell. The performance of the devices was reproducible and stable for a period of at least 3 weeks. We also report first external and internal quantum efficiency measurements for GM SSCs, which point to possible paths for further performance improvements.
Collapse
|
45
|
Adamska L, Nayyar I, Chen H, Swan AK, Oldani N, Fernandez-Alberti S, Golder MR, Jasti R, Doorn SK, Tretiak S. Self-trapping of excitons, violation of Condon approximation, and efficient fluorescence in conjugated cycloparaphenylenes. NANO LETTERS 2014; 14:6539-6546. [PMID: 25310514 DOI: 10.1021/nl503133e] [Citation(s) in RCA: 119] [Impact Index Per Article: 11.9] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/04/2023]
Abstract
Cycloparaphenylenes, the simplest structural unit of armchair carbon nanotubes, have unique optoelectronic properties counterintuitive in the class of conjugated organic materials. Our time-dependent density functional theory study and excited state dynamics simulations of cycloparaphenylene chromophores provide a simple and conceptually appealing physical picture explaining experimentally observed trends in optical properties in this family of molecules. Fully delocalized degenerate second and third excitonic states define linear absorption spectra. Self-trapping of the lowest excitonic state due to electron-phonon coupling leads to the formation of spatially localized excitation in large cycloparaphenylenes within 100 fs. This invalidates the commonly used Condon approximation and breaks optical selection rules, making these materials superior fluorophores. This process does not occur in the small molecules, which remain inefficient emitters. A complex interplay of symmetry, π-conjugation, conformational distortion and bending strain controls all photophysics of cycloparaphenylenes.
Collapse
|
46
|
Ma X, Roslyak O, Wang F, Duque JG, Piryatinski A, Doorn SK, Htoon H. Influence of exciton dimensionality on spectral diffusion of single-walled carbon nanotubes. ACS NANO 2014; 8:10613-20. [PMID: 25251324 DOI: 10.1021/nn504138m] [Citation(s) in RCA: 1] [Impact Index Per Article: 0.1] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 05/12/2023]
Abstract
We study temporal evolution of photoluminescence (PL) spectra from individual single-walled carbon nanotubes (SWCNTs) at cryogenic and room temperatures. Sublinear and superlinear correlations between fluctuating PL spectral positions and line widths are observed at cryogenic and room temperatures, respectively. We develop a simple model to explain these two different spectral diffusion behaviors in the framework of quantum-confined Stark effect (QCSE) caused by surface charges trapped in the vicinity of SWCNTs. We show that the wave function properties of excitons, namely, localization at cryogenic temperature and delocalization at room temperature, play a critical role in defining sub- and superlinear correlations. Room temperature PL spectral positions and line widths of SWCNTs coupled to gold dimer nanoantennas on the other hand exhibit sublinear correlations, indicating that excitonic emission mainly originates from nanometer range regions and excitons appear to be localized. Our numerical simulations show that such apparent localization of excitons results from plasmonic confinement of excitation and an enhancement of decay rates in the gap of the dimer nanoantennas.
Collapse
|
47
|
Ma X, Adamska L, Yamaguchi H, Yalcin SE, Tretiak S, Doorn SK, Htoon H. Electronic structure and chemical nature of oxygen dopant states in carbon nanotubes. ACS NANO 2014; 8:10782-9. [PMID: 25265272 DOI: 10.1021/nn504553y] [Citation(s) in RCA: 70] [Impact Index Per Article: 7.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 05/18/2023]
Abstract
We performed low temperature photoluminescence (PL) studies on individual oxygen-doped single-walled carbon nanotubes (SWCNTs) and correlated our observations to electronic structure simulations. Our experiment reveals multiple sharp asymmetric emission peaks at energies 50-300 meV red-shifted from that of the E11 bright exciton peak. Our simulation suggests an association of these peaks with deep trap states tied to different specific chemical adducts. In addition, oxygen doping is also observed to split the E11 exciton into two or more states with an energy splitting <40 meV. We attribute these states to dark states that are brightened through defect-induced symmetry breaking. While the wave functions of these brightened states are delocalized, those of the deep-trap states are strongly localized and pinned to the dopants. These findings are consistent with our experimental observation of asymmetric broadening of the deep trap emission peaks, which can result from interaction between pinned excitons and one-dimensional phonons. Exciton pinning also increases the sensitivity of the deep traps to the local dielectric environment, leading to a large inhomogeneous broadening. Observations of multiple spectral features on single nanotubes indicate the possibility of different chemical adducts coexisting on a given nanotube.
Collapse
|
48
|
Lim YS, Nugraha ART, Cho SJ, Noh MY, Yoon EJ, Liu H, Kim JH, Telg H, Hároz EH, Sanders GD, Baik SH, Kataura H, Doorn SK, Stanton CJ, Saito R, Kono J, Joo T. Ultrafast generation of fundamental and multiple-order phonon excitations in highly enriched (6,5) single-wall carbon nanotubes. NANO LETTERS 2014; 14:1426-1432. [PMID: 24527806 DOI: 10.1021/nl404536b] [Citation(s) in RCA: 12] [Impact Index Per Article: 1.2] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/03/2023]
Abstract
Using a macroscopic ensemble of highly enriched (6,5) single-wall carbon nanotubes, combined with high signal-to-noise ratio and time-dependent differential transmission spectroscopy, we have generated vibrational modes in an ultrawide spectral range (10-3000 cm(-1)). A total of 14 modes were clearly resolved and identified, including fundamental modes of A, E1, and E2 symmetries and their combinational modes involving two and three phonons. Through comparison with continuous wave Raman spectra as well as calculations based on an extended tight-binding model, we were able to identify all the observed peaks and determine the frequencies of the individual and combined modes. We provide a full summary of phonon frequencies for (6,5) nanotubes that can serve as a basic reference with which to refine our understanding of nanotube phonon spectra as well as a testbed for new theoretical models.
Collapse
|
49
|
Subbaiyan NK, Cambré S, Parra-Vasquez ANG, Hároz EH, Doorn SK, Duque JG. Role of surfactants and salt in aqueous two-phase separation of carbon nanotubes toward simple chirality isolation. ACS NANO 2014; 8:1619-28. [PMID: 24450507 DOI: 10.1021/nn405934y] [Citation(s) in RCA: 99] [Impact Index Per Article: 9.9] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 05/12/2023]
Abstract
Aqueous two-phase extraction has recently been demonstrated as a new method to separate single-wall carbon nanotubes (SWCNTs). In this work, we determined that the mechanism of separation is driven by the hydrophobicity of the surfactant, or combination of surfactants, at the SWCNT surface. This knowledge allowed us to develop a simple approach for obtaining highly enriched single-chirality suspensions in only 1 or 2 steps. These results were obtained by strategically combining multiple surfactants with different diameter-dependent binding affinities for SWCNTs and salts that readjust the surfactant structure within the mixed micelle surrounding the SWCNTs. The procedure is successfully applied to SWCNTs from different sources (CoMoCAT and HiPco) with various diameter distributions (from 0.53 to 1.2 nm). Each separation step is characterized by optical absorption, resonant Raman, and photoluminescence excitation spectroscopies. By determining the SWCNT sorting mechanism, we were able to develop a new set of parameters that separated another chirality.
Collapse
|
50
|
Berciaud S, Li X, Htoon H, Brus LE, Doorn SK, Heinz TF. Intrinsic line shape of the Raman 2D-mode in freestanding graphene monolayers. NANO LETTERS 2013; 13:3517-3523. [PMID: 23799800 DOI: 10.1021/nl400917e] [Citation(s) in RCA: 25] [Impact Index Per Article: 2.3] [Reference Citation Analysis] [Abstract] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/02/2023]
Abstract
We report a comprehensive study of the two-phonon intervalley (2D) Raman mode in graphene monolayers, motivated by recent reports of asymmetric 2D-mode line shapes in freestanding graphene. For photon energies in the range 1.53-2.71 eV, the 2D-mode Raman response of freestanding samples appears as bimodal, in stark contrast with the Lorentzian approximation that is commonly used for supported monolayers. The transition between the freestanding and supported cases is mimicked by electrostatically doping freestanding graphene at carrier densities above 2 × 10(11) cm(-2). This result quantitatively demonstrates that low levels of charging can obscure the intrinsically bimodal 2D-mode line shape of monolayer graphene. In pristine freestanding graphene, we observe a broadening of the 2D-mode feature with decreasing photon energy that cannot be rationalized using a simple one-dimensional model based on resonant inner and outer processes. This indicates that phonon wavevectors away from the high-symmetry lines of the Brillouin zone must contribute to the 2D-mode, so that a full two-dimensional calculation is required to properly describe multiphonon-resonant Raman processes.
Collapse
|