1
|
Virág ÁD, Tóth C, Polyák P, Musioł M, Molnár K. Tailoring the mechanical and rheological properties of poly(lactic acid) by sterilizing UV-C irradiation. Int J Biol Macromol 2024; 277:134247. [PMID: 39142990 DOI: 10.1016/j.ijbiomac.2024.134247] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 03/28/2024] [Revised: 07/23/2024] [Accepted: 07/27/2024] [Indexed: 08/16/2024]
Abstract
In this study, we irradiated amorphous (A) and semi-crystalline (SC) poly(lactic acid) (PLA) with different UV-C doses up to 2214 kJ/m2. We achieved an average crystallinity of 43 % by heat treatment, which was unaffected by UV-C irradiation. Modulated differential scanning calorimetry showed that crystal polymorphs and the ratio of rigid amorphous and mobile amorphous phases were also unaffected. Using gel permeation chromatography analysis, we showed that the degradation mechanism was noncatalytic random scission, and the initial molar mass was reduced by >90 % at a dose of 2214 kJ/m2 for both A- and SC-PLA samples. Our Raman spectroscopy results indicated that the probability of the formation of oxygen-containing groups increases with increasing UV-C doses. Since we found that the mechanical properties of PLA films can be tailored with UV-C light, we proposed a method to predict the overall tensile curve as a function of the UV-C dose. We also proposed a modified Cross-WLF model to describe the effect of UV-C irradiation on viscosity up to 55 % molar mass reduction. The models allow us to estimate the limits of recyclability and reusability of sterilised PLA products.
Collapse
Affiliation(s)
- Ábris Dávid Virág
- Department of Polymer Engineering, Faculty of Mechanical Engineering, Budapest University of Technology and Economics, Műegyetem rkp. 3. H-1111 Budapest, Hungary.
| | - Csenge Tóth
- Department of Polymer Engineering, Faculty of Mechanical Engineering, Budapest University of Technology and Economics, Műegyetem rkp. 3. H-1111 Budapest, Hungary; MTA-BME Lendület Lightweight Polymer Composites Research Group, Műegyetem rkp. 3, H-1111 Budapest, Hungary.
| | - Péter Polyák
- Department of Food, Agricultural and Biological Engineering, College of Food, Agricultural, and Environmental Sciences, The Ohio State University, 1680 Madison Avenue, 44691 Wooster, OH, USA; Laboratory of Plastics and Rubber Technology, Department of Physical Chemistry and Materials Science, Faculty of Chemical Technology and Biotechnology, Budapest University of Technology and Economics, Műegyetem rkp. 3. H-1111 Budapest, Hungary.
| | - Marta Musioł
- Centre of Polymer and Carbon Materials, Polish Academy of Sciences, 34, M. Curie-Skłodowska St, 41-819 Zabrze, Poland.
| | - Kolos Molnár
- Department of Polymer Engineering, Faculty of Mechanical Engineering, Budapest University of Technology and Economics, Műegyetem rkp. 3. H-1111 Budapest, Hungary; HUN-REN-BME Research Group for Composite Science and Technology, Műegyetem rkp. 3, H-1111 Budapest, Hungary.
| |
Collapse
|
2
|
Dobrzyńska-Mizera M, Dodda JM, Liu X, Knitter M, Oosterbeek RN, Salinas P, Pozo E, Ferreira AM, Sadiku ER. Engineering of Bioresorbable Polymers for Tissue Engineering and Drug Delivery Applications. Adv Healthc Mater 2024:e2401674. [PMID: 39233521 DOI: 10.1002/adhm.202401674] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Grants] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 05/06/2024] [Revised: 08/15/2024] [Indexed: 09/06/2024]
Abstract
Herein, the recent advances in the development of resorbable polymeric-based biomaterials, their geometrical forms, resorption mechanisms, and their capabilities in various biomedical applications are critically reviewed. A comprehensive discussion of the engineering approaches for the fabrication of polymeric resorbable scaffolds for tissue engineering, drug delivery, surgical, cardiological, aesthetical, dental and cardiovascular applications, are also explained. Furthermore, to understand the internal structures of resorbable scaffolds, representative studies of their evaluation by medical imaging techniques, e.g., cardiac computer tomography, are succinctly highlighted. This approach provides crucial clinical insights which help to improve the materials' suitable and viable characteristics for them to meet the highly restrictive medical requirements. Finally, the aspects of the legal regulations and the associated challenges in translating research into desirable clinical and marketable materials of polymeric-based formulations, are presented.
Collapse
Affiliation(s)
- Monika Dobrzyńska-Mizera
- Institute of Materials Technology, Polymer Division, Poznan University of Technology, Poznan, Poland
| | - Jagan Mohan Dodda
- New Technologies - Research Centre (NTC), University of West Bohemia, Univerzitní 8, Pilsen, 30100, Czech Republic
| | - Xiaohua Liu
- Chemical and Biomedical Engineering Department, University of Missouri, 1030 Hill Street, Columbia, Missouri, 65211, USA
| | - Monika Knitter
- Institute of Materials Technology, Polymer Division, Poznan University of Technology, Poznan, Poland
| | - Reece N Oosterbeek
- Department of Engineering Science, University of Oxford, Parks Road, Oxford, OX1 3PJ, UK
| | - Pablo Salinas
- Department of Cardiology, Hospital Clínico San Carlos, Madrid, Spain
- Instituto de Investigación Sanitaria del Hospital Clínico San Carlos (IdISSC), Madrid, Spain
| | - Eduardo Pozo
- Department of Cardiology, Hospital Clínico San Carlos, Madrid, Spain
- Instituto de Investigación Sanitaria del Hospital Clínico San Carlos (IdISSC), Madrid, Spain
| | - Ana Marina Ferreira
- School of Engineering, Newcastle University, Newcastle upon Tyne, Newcastle, NE1 7RU, UK
| | - Emmanuel Rotimi Sadiku
- Tshwane University of Technology, Department of Chemical, Metallurgical and Materials Engineering, Polymer Division & Institute for Nano Engineering Research (INER), Pretoria West Campus, Pretoria, South Africa
| |
Collapse
|
3
|
Wang L, Tu Z, Liang J, Wei Z. Poly(butylene oxalate-co-terephthalate): A PBAT-like but rapid hydrolytic degradation plastic. JOURNAL OF HAZARDOUS MATERIALS 2024; 471:134349. [PMID: 38653140 DOI: 10.1016/j.jhazmat.2024.134349] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Received: 02/05/2024] [Revised: 03/28/2024] [Accepted: 04/17/2024] [Indexed: 04/25/2024]
Abstract
Concerns over worldwide plastic pollution have led to the development of biodegradable polyester materials with excellent physical and chemical properties through the copolymerization of poly(butylene oxalate) (PBOx). As a result, poly(butylene oxalate-co-terephthalate)s (PBOTs) with varying compositions, were prepared by incorporating aromatic units. Studies have indicated that PBOT-47 (with a 47% molar terephthalate), exhibits exceptional mechanical properties. With an elongation at break of 1160% and a tensile strength that remains above 30 MPa, similar to or even better than those of the commercial biodegradable plastic poly(butylene adipate-co-terephthalate) PBAT-47 (47% molar terephthalate). Moreover, the permeability coefficients of PBAT-47 for H2O, CO2 and O2 were 5.8, 50.6 and 5.6 times higher than that of PBOT-47, revealing the superior barrier properties of PBOT. Through experimental research and theoretical simulation, the mechanism of the copolymer hydrolysis was elucidated. The readily hydrolytic nature of the oxalate unit endows it with the capacity for rapid degradation, possessing the potential to be a short-term degradable material with physical properties similar to PBAT.
Collapse
Affiliation(s)
- Lizheng Wang
- State Key Laboratory of Fine Chemicals, Liaoning Key Laboratory of Polymer Science and Engineering, Department of Polymer Science and Engineering, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China
| | - Zhu Tu
- State Key Laboratory of Fine Chemicals, Liaoning Key Laboratory of Polymer Science and Engineering, Department of Polymer Science and Engineering, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China
| | - Jiaming Liang
- State Key Laboratory of Fine Chemicals, Liaoning Key Laboratory of Polymer Science and Engineering, Department of Polymer Science and Engineering, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China
| | - Zhiyong Wei
- State Key Laboratory of Fine Chemicals, Liaoning Key Laboratory of Polymer Science and Engineering, Department of Polymer Science and Engineering, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China.
| |
Collapse
|
4
|
Hallstein J, Metzsch-Zilligen E, Pfaendner R. Long-Term Thermal Stabilization of Poly(Lactic Acid). MATERIALS (BASEL, SWITZERLAND) 2024; 17:2761. [PMID: 38894026 PMCID: PMC11173481 DOI: 10.3390/ma17112761] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Grants] [Track Full Text] [Subscribe] [Scholar Register] [Received: 05/06/2024] [Revised: 05/28/2024] [Accepted: 05/31/2024] [Indexed: 06/21/2024]
Abstract
To use polylactic acid in demanding technical applications, sufficient long-term thermal stability is required. In this work, the thermal aging of polylactic acid (PLA) in the solid phase at 100 °C and 150 °C is investigated. PLA has only limited aging stability without the addition of stabilizers. Therefore, the degradation mechanism in thermal aging was subsequently investigated in more detail to identify a suitable stabilization strategy. Investigations using nuclear magnetic resonance spectroscopy showed that, contrary to expectations, even under thermal aging conditions, hydrolytic degradation rather than oxidative degradation is the primary degradation mechanism. This was further confirmed by the investigation of suitable stabilizers. While the addition of phenols, phosphites and thioethers as antioxidants leads only to a limited improvement in aging stability, the addition of an additive composition to provide hydrolytic stabilization results in extended durability. Efficient compositions consist of an aziridine-based hydrolysis inhibitor and a hydrotalcite co-stabilizer. At an aging temperature of 100 °C, the time until significant polymer chain degradation occurs is extended from approx. 500 h for unstabilized polylactic acid to over 2000 h for stabilized polylactic acid.
Collapse
Affiliation(s)
| | | | - Rudolf Pfaendner
- Division Plastics, Fraunhofer Institute for Structural Durability and System Reliability LBF, 64289 Darmstadt, Germany; (J.H.); (E.M.-Z.)
| |
Collapse
|
5
|
He S, Wei L, Wang G, Pugno NM, Chen Q, Li Z. In Silico Evaluation of In Vivo Degradation Kinetics of Poly(Lactic Acid) Vascular Stent Devices. J Funct Biomater 2024; 15:135. [PMID: 38786646 PMCID: PMC11122488 DOI: 10.3390/jfb15050135] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Grants] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 03/28/2024] [Revised: 05/09/2024] [Accepted: 05/11/2024] [Indexed: 05/25/2024] Open
Abstract
Biodegradable vascular stents (BVS) are deemed as great potential alternatives for overcoming the inherent limitations of permanent metallic stents in the treatment of coronary artery diseases. The current study aimed to comprehensively compare the mechanical behaviors of four poly(lactic acid) (PLA) BVS designs with varying geometries via numerical methods and to clarify the optimal BVS selection. Four PLA BVS (i.e., Absorb, DESolve, Igaki-Tamai, and Fantom) were first constructed. A degradation model was refined by simply including the fatigue effect induced by pulsatile blood pressures, and an explicit solver was employed to simulate the crimping and degradation behaviors of the four PLA BVS. The degradation dynamics here were characterized by four indices. The results indicated that the stent designs affected crimping and degradation behaviors. Compared to the other three stents, the DESolve stent had the greatest radial stiffness in the crimping simulation and the best diameter maintenance ability despite its faster degradation; moreover, the stent was considered to perform better according to a pilot scoring system. The current work provides a theoretical method for studying and understanding the degradation dynamics of the PLA BVS, and it could be helpful for the design of next-generation BVS.
Collapse
Affiliation(s)
- Shicheng He
- Biomechanics Laboratory, School of Biological Science and Medical Engineering, Southeast University, Nanjing 210096, China
| | - Lingling Wei
- School of Food and Biological Engineering, Hefei University of Technology, Hefei 230601, China
| | - Guixue Wang
- Key Laboratory for Biorheological Science and Technology of Ministry of Education, State and Local Joint Engineering Laboratory for Vascular Implants, Bioengineering College of Chongqing University, Chongqing 400030, China
| | - Nicola M. Pugno
- Laboratory for Bioinspired, Bionic, Nano, Meta Materials and Mechanics, University of Trento, Via Mesiano 77, 38123 Trento, Italy
- School of Engineering and Materials Science, Queen Mary University of London, Mile End Road, London E1 4NS, UK
| | - Qiang Chen
- Biomechanics Laboratory, School of Biological Science and Medical Engineering, Southeast University, Nanjing 210096, China
| | - Zhiyong Li
- Biomechanics Laboratory, School of Biological Science and Medical Engineering, Southeast University, Nanjing 210096, China
- School of Mechanical, Medical and Process Engineering, Queensland University of Technology, Brisbane, QLD 4001, Australia
- Faculty of Sports Science, Ningbo University, Ningbo 315211, China
| |
Collapse
|
6
|
Havlickova K, Kuzelova Kostakova E, Lisnenko M, Hauzerova S, Stuchlik M, Vrchovecka S, Vistejnova L, Molacek J, Lukas D, Prochazkova R, Horakova J, Jakubkova S, Heczkova B, Jencova V. The Impacts of the Sterilization Method and the Electrospinning Conditions of Nanofibrous Biodegradable Layers on Their Degradation and Hemocompatibility Behavior. Polymers (Basel) 2024; 16:1029. [PMID: 38674949 PMCID: PMC11053452 DOI: 10.3390/polym16081029] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Grants] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 03/08/2024] [Revised: 03/26/2024] [Accepted: 04/04/2024] [Indexed: 04/28/2024] Open
Abstract
The use of electrospun polymeric biodegradable materials for medical applications is becoming increasingly widespread. One of the most important parameters regarding the functionality of nanofiber scaffolds during implantation and the subsequent regeneration of damaged tissues concerns their stability and degradation behavior, both of which are influenced by a wide range of factors (the properties of the polymer and the polymer solution, the technological processing approach, the sterilization method, etc.). This study monitored the degradation of nanofibrous materials fabricated from degradable polyesters as a result of the sterilization method applied (ethylene oxide and gamma irradiation) and the solvent system used to prepare the spun polymer solution. Aliphatic polyesters PCL and PLCL were chosen for this study and selected with respect to the applicability and handling in the surgical setting of these nanofibrous materials for vascular bandaging. The results revealed that the choice of solvent system exerts a significant impact on degradation during sterilization, especially at higher gamma irradiation values. The subsequent enzyme-catalyzed degradation of the materials following sterilization indicated that the choice of the sterilization method influenced the degradation behavior of the materials. Whereas wave-like degradation was evident concerning ethylene oxide sterilization, no such behavior was observed following gamma-irradiation sterilization. With concern for some of the tested materials, the results also indicated the potential for influencing the development of degradation within the bulk versus degradation from the surface of the material. Both the sterilization method and the choice of the spinning solvent system were found to impact degradation, which was observed to be most accelerated in the case of PLCL (L-lactide-co-caprolactone copolymer) electrospun from organic acids and subsequently sterilized using gamma irradiation. Since we planned to use these materials in cardiovascular applications, it was decided that their hemocompatibility would also be tested. The results of these tests revealed that changes in the structures of the materials initiated by sterilization may exert thrombogenic and anticoagulant impacts. Moreover, the microscopic analysis suggested that the solvent system used in the preparation of the materials potentially affects the behavior of erythrocytes; however, no indication of the occurrence of hemolysis was detected.
Collapse
Affiliation(s)
- Kristyna Havlickova
- Department of Chemistry, Faculty of Science, Humanities and Education, Technical University of Liberec, Studentská 1402/2, 46117 Liberec, Czech Republic; (M.L.); (S.H.); (D.L.); (V.J.)
| | - Eva Kuzelova Kostakova
- Department of Chemistry, Faculty of Science, Humanities and Education, Technical University of Liberec, Studentská 1402/2, 46117 Liberec, Czech Republic; (M.L.); (S.H.); (D.L.); (V.J.)
| | - Maxim Lisnenko
- Department of Chemistry, Faculty of Science, Humanities and Education, Technical University of Liberec, Studentská 1402/2, 46117 Liberec, Czech Republic; (M.L.); (S.H.); (D.L.); (V.J.)
| | - Sarka Hauzerova
- Department of Chemistry, Faculty of Science, Humanities and Education, Technical University of Liberec, Studentská 1402/2, 46117 Liberec, Czech Republic; (M.L.); (S.H.); (D.L.); (V.J.)
| | - Martin Stuchlik
- Institute for Nanomaterials, Advanced Technology and Innovation, Technical University of Liberec, Bendlova 1409/7, 46117 Liberec, Czech Republic; (M.S.); (S.V.)
| | - Stanislava Vrchovecka
- Institute for Nanomaterials, Advanced Technology and Innovation, Technical University of Liberec, Bendlova 1409/7, 46117 Liberec, Czech Republic; (M.S.); (S.V.)
| | - Lucie Vistejnova
- Biomedical Center, Faculty of Medicine in Pilsen, Charles University, Alej Svobody 1655/76, 32300 Pilsen, Czech Republic; (L.V.); (J.M.)
| | - Jiri Molacek
- Biomedical Center, Faculty of Medicine in Pilsen, Charles University, Alej Svobody 1655/76, 32300 Pilsen, Czech Republic; (L.V.); (J.M.)
- Department of Surgery, Faculty of Medicine in Pilsen, Charles University, Alej Svobody 80, 32300 Pilsen, Czech Republic
| | - David Lukas
- Department of Chemistry, Faculty of Science, Humanities and Education, Technical University of Liberec, Studentská 1402/2, 46117 Liberec, Czech Republic; (M.L.); (S.H.); (D.L.); (V.J.)
| | - Renata Prochazkova
- Regional Hospital Liberec, Husova 357/28, 46001 Liberec, Czech Republic; (R.P.); (S.J.); (B.H.)
- Institute of Clinical Disciplines and Biomedicine, Faculty of Health Studies, Technical University of Liberec, Studentská 1402/2, 46117 Liberec, Czech Republic
| | - Jana Horakova
- Department of Nonwovens and Nanofibrous Materials, Faculty of Textile Engineering, Technical University of Liberec, Studentská 1402/2, 46117 Liberec, Czech Republic;
| | - Sarka Jakubkova
- Regional Hospital Liberec, Husova 357/28, 46001 Liberec, Czech Republic; (R.P.); (S.J.); (B.H.)
| | - Bohdana Heczkova
- Regional Hospital Liberec, Husova 357/28, 46001 Liberec, Czech Republic; (R.P.); (S.J.); (B.H.)
| | - Vera Jencova
- Department of Chemistry, Faculty of Science, Humanities and Education, Technical University of Liberec, Studentská 1402/2, 46117 Liberec, Czech Republic; (M.L.); (S.H.); (D.L.); (V.J.)
| |
Collapse
|
7
|
Abaei AR, Shine CJ, Vaughan TJ, Ronan W. An integrated mechanical degradation model to explore the mechanical response of a bioresorbable polymeric scaffold. J Mech Behav Biomed Mater 2024; 152:106419. [PMID: 38325169 DOI: 10.1016/j.jmbbm.2024.106419] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 10/31/2023] [Revised: 01/17/2024] [Accepted: 01/23/2024] [Indexed: 02/09/2024]
Abstract
Simulation of bioresorbable medical devices is hindered by the limitations of current material models. Useful simulations require that both the short- and long-term response must be considered; existing models are not physically-based and provide limited insight to guide performance improvements. This study presents an integrated degradation framework which couples a physically-based degradation model, which predicts changes in both crystallinity (Xc) and molecular weight (Mn), with the results of a micromechanical model, which predicts the effective properties of the semicrystalline polymer. This degradation framework is used to simulate the deployment of a bioresorbable PLLA (Poly (L-lactide) stent into a mock vessel and the subsequent mechanical response during degradation under different diffusion boundary conditions representing neointimal growth. A workflow is established in a commercial finite element code that couples both the immediate and long-term responses. Clinically relevant lumen loss is reported and used to compare different responses and the effect of neo-intimal tissue regrowth post-implantation on degradation and on the mechanical response is assessed. In addition, the effects of possible changes in Xc, which could occur during processing and stent deployment, are explored.
Collapse
Affiliation(s)
- A R Abaei
- Biomechanics Research Centre (BMEC), Biomedical Engineering, School of Engineering, University of Galway, Ireland
| | - Connor J Shine
- Biomechanics Research Centre (BMEC), Biomedical Engineering, School of Engineering, University of Galway, Ireland
| | - T J Vaughan
- Biomechanics Research Centre (BMEC), Biomedical Engineering, School of Engineering, University of Galway, Ireland
| | - W Ronan
- Biomechanics Research Centre (BMEC), Biomedical Engineering, School of Engineering, University of Galway, Ireland.
| |
Collapse
|
8
|
Koons GL, Kontoyiannis PD, Diaz-Gomez L, Elsarrag SZ, Scott DW, Diba M, Mikos AG. Influence of Polymeric Microparticle Size and Loading Concentration on 3D Printing Accuracy and Degradation Behavior of Composite Scaffolds. 3D PRINTING AND ADDITIVE MANUFACTURING 2024; 11:e813-e827. [PMID: 38694834 PMCID: PMC11058418 DOI: 10.1089/3dp.2022.0208] [Citation(s) in RCA: 2] [Impact Index Per Article: 2.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 05/04/2024]
Abstract
Successful employment of 3D printing for delivery of therapeutic biomolecules requires protection of their bioactivity on exposure to potentially inactivating conditions. Although intermediary encapsulation of the biomolecules in polymeric particulate delivery vehicles is a promising strategy for this objective, the inclusion of such particles in 3D printing formulations may critically impact the accuracy or precision of 3D printed scaffolds relative to their intended designed architectures, as well as the degradation behavior of both the scaffolds and the included particles. The present work aimed to elucidate the effect of poly(d,l-lactic-co-glycolic acid) particle size and loading concentration on material accuracy, machine precision, and degradation of 3D printed poly(ɛ-caprolactone)-based scaffolds. Using a main effects analysis, the sizes and loading concentrations of particle delivery vehicles investigated were found to have neither a beneficial nor disadvantageous influence on the metrics of printing quality such as material accuracy and machine precision. Meanwhile, particle loading concentration was determined to influence degradation rate, whereas printing temperature affected the trends in composite weight-average molecular weight. Neither of the two particle-related parameters (concentration nor diameter) was found to exhibit a significant effect on intra-fiber nor inter-fiber porosity. These findings evidence the capacity for controlled loading of particulate delivery vehicles in 3D printed scaffolds while preserving construct accuracy and precision, and with predictable dictation of composite degradation behavior for potential controlled release of encapsulated biomolecules.
Collapse
Affiliation(s)
- Gerry L. Koons
- Department of Bioengineering, Rice University, Houston, Texas, USA
- Medical Scientist Training Program, Baylor College of Medicine, Houston, Texas, USA
| | - Panayiotis D. Kontoyiannis
- Department of Bioengineering, Rice University, Houston, Texas, USA
- McGovern Medical School, The University of Texas Health Science Center at Houston, Houston, Texas, USA
| | - Luis Diaz-Gomez
- Department of Pharmacology, Pharmacy, and Pharmaceutical Technology, Universidade de Santiago de Compostela, Santiago de Compostela, Spain
| | - Selma Z. Elsarrag
- Department of Bioengineering, Rice University, Houston, Texas, USA
- Department of Quantitative and Computational Biology, Baylor College of Medicine, Houston, Texas, USA
| | - David W. Scott
- Department of Statistics, Rice University, Houston, Texas, USA
| | - Mani Diba
- Department of Bioengineering, Rice University, Houston, Texas, USA
| | | |
Collapse
|
9
|
Virág ÁD, Tóth C, Molnár K. Photodegradation of polylactic acid: Characterisation of glassy and melt behaviour as a function of molecular weight. Int J Biol Macromol 2023; 252:126336. [PMID: 37586636 DOI: 10.1016/j.ijbiomac.2023.126336] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 06/10/2023] [Revised: 07/28/2023] [Accepted: 08/12/2023] [Indexed: 08/18/2023]
Abstract
During the COVID-19 pandemic, UV-C germicidal lamps became widely available, even for household applications. However, their long-term degradation effects on the mechanical and rheological properties of polylactic acid (PLA) are still not well established. The relationship between degradation and its effects on the molecular structure and macroscale properties are hardly known. In this study, we investigated the effects of long-term exposure to UV-C irradiation on the properties of PLA and interpreted the results at the molecular scale. We performed gel permeation chromatography, Fourier-transform infrared spectroscopy and UV-Vis spectroscopy to analyse changes in chemical structure induced by the UV-irradiation. Then, we carried out thermal, rheological and tensile tests to investigate mechanical and melting properties, and we investigated the applicability of these test results to estimate molecular weight loss. We have created a 3D irradiation map that can facilitate the design of disinfection devices. Based on our results, we propose a maximum number of sterilisation cycles (13 cycles) for the tested PLA films that do not result in significant changes in tensile strength and modulus.
Collapse
Affiliation(s)
- Ábris Dávid Virág
- Department of Polymer Engineering, Faculty of Mechanical Engineering, Budapest University of Technology and Economics, Műegyetem rkp. 3. H-1111 Budapest, Hungary.
| | - Csenge Tóth
- Department of Polymer Engineering, Faculty of Mechanical Engineering, Budapest University of Technology and Economics, Műegyetem rkp. 3. H-1111 Budapest, Hungary.
| | - Kolos Molnár
- Department of Polymer Engineering, Faculty of Mechanical Engineering, Budapest University of Technology and Economics, Műegyetem rkp. 3. H-1111 Budapest, Hungary; ELKH-BME Research Group for Composite Science and Technology, Műegyetem rkp. 3., H-1111 Budapest, Hungary.
| |
Collapse
|
10
|
Giolando PA, Hopkins K, Davis BF, Vike N, Ahmadzadegan A, Ardekani AM, Vlachos PP, Rispoli JV, Solorio L, Kinzer-Ursem TL. Mechanistic Computational Modeling of Implantable, Bioresorbable Drug Release Systems. ADVANCED MATERIALS (DEERFIELD BEACH, FLA.) 2023; 35:e2301698. [PMID: 37243452 PMCID: PMC10697660 DOI: 10.1002/adma.202301698] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Grants] [Track Full Text] [Subscribe] [Scholar Register] [Received: 02/21/2023] [Revised: 05/09/2023] [Indexed: 05/28/2023]
Abstract
Implantable, bioresorbable drug delivery systems offer an alternative to current drug administration techniques; allowing for patient-tailored drug dosage, while also increasing patient compliance. Mechanistic mathematical modeling allows for the acceleration of the design of the release systems, and for prediction of physical anomalies that are not intuitive and may otherwise elude discovery. This study investigates short-term drug release as a function of water-mediated polymer phase inversion into a solid depot within hours to days, as well as long-term hydrolysis-mediated degradation and erosion of the implant over the next few weeks. Finite difference methods are used to model spatial and temporal changes in polymer phase inversion, solidification, and hydrolysis. Modeling reveals the impact of non-uniform drug distribution, production and transport of H+ ions, and localized polymer degradation on the diffusion of water, drug, and hydrolyzed polymer byproducts. Compared to experimental data, the computational model accurately predicts the drug release during the solidification of implants over days and drug release profiles over weeks from microspheres and implants. This work offers new insight into the impact of various parameters on drug release profiles, and is a new tool to accelerate the design process for release systems to meet a patient specific clinical need.
Collapse
Affiliation(s)
- Patrick A Giolando
- Weldon School of Biomedical Engineering, Purdue University, West Lafayette, IN, 47907, USA
- School of Mechanical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Kelsey Hopkins
- Weldon School of Biomedical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Barrett F Davis
- Weldon School of Biomedical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Nicole Vike
- Weldon School of Biomedical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Adib Ahmadzadegan
- School of Mechanical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Arezoo M Ardekani
- School of Mechanical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Pavlos P Vlachos
- Weldon School of Biomedical Engineering, Purdue University, West Lafayette, IN, 47907, USA
- School of Mechanical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Joseph V Rispoli
- Weldon School of Biomedical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Luis Solorio
- Weldon School of Biomedical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| | - Tamara L Kinzer-Ursem
- Weldon School of Biomedical Engineering, Purdue University, West Lafayette, IN, 47907, USA
| |
Collapse
|
11
|
Pan Z, Brassart L. A reaction-diffusion framework for hydrolytic degradation of amorphous polymers based on a discrete chain scission model. Acta Biomater 2023:S1742-7061(23)00346-X. [PMID: 37343906 DOI: 10.1016/j.actbio.2023.06.021] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 02/15/2023] [Revised: 06/06/2023] [Accepted: 06/15/2023] [Indexed: 06/23/2023]
Abstract
Hydrolytic degradation of polymers involves the scission of long chain molecules, leading to molecular weight reduction and mass loss. The precise degradation response however depends on the scission probability of individual bonds along the polymer backbone. In particular, bonds near the chain ends are considered to be more susceptible to hydrolysis than inner bonds. In this paper, we incorporate a discrete chain scission model that can handle arbitrary bond scission probabilities within a continuum reaction-diffusion framework. Overall hydrolysis kinetics (including autocatalysis) is described independently of the chain scission model. By decoupling the description of the chain scission mechanism from kinetics, our framework enables the identification of the chain scission mechanism from molecular weight reduction and mass loss curves commonly reported in experimental degradation studies. We further propose a reduced continuum model which is better suited for large-scale simulations while retaining the predictive capability of the full discrete-continuum model. The model capability is illustrated in representative case studies based on experimental data from the literature for different materials and geometries. STATEMENT OF SIGNIFICANCE: Many models have been proposed to predict the evolution of molecular weight and mass loss in biodegradable polymers undergoing hydrolytic degradation. However, existing models remain limited in their ability to describe the degradation mechanism, autocatalytic kinetics and short chains diffusion simultaneously. Moreover, existing models often rely on empirical relations and a large number of fitting parameters. Here, we propose a conceptually simple discrete-continuum mathematical framework with a small number of parameters which all have a clear physical meaning. Model calibration against experimental data is simplified, and further provides insights into the degradation mechanisms at play, namely random scission, chain-end scission, or a combination of both. The framework can serve as a basis for future generalisations, including a description of evolving crystallinity, or other degradation mechanisms, such as thermal oxidation or photo-degradation.
Collapse
Affiliation(s)
- Zhouzhou Pan
- Department of Engineering Science, University of Oxford, Oxford OX1 3PJ, UK
| | - Laurence Brassart
- Department of Engineering Science, University of Oxford, Oxford OX1 3PJ, UK.
| |
Collapse
|
12
|
Wu F, Guo Z, Cui K, Dong D, Yang X, Li J, Wu Z, Li L, Dai Y, Pan T. Insights into characteristics of white rot fungus during environmental plastics adhesion and degradation mechanism of plastics. JOURNAL OF HAZARDOUS MATERIALS 2023; 448:130878. [PMID: 36731319 DOI: 10.1016/j.jhazmat.2023.130878] [Citation(s) in RCA: 13] [Impact Index Per Article: 13.0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Subscribe] [Scholar Register] [Received: 12/01/2022] [Revised: 01/17/2023] [Accepted: 01/25/2023] [Indexed: 06/18/2023]
Abstract
Since the 1980s, plastic waste in the environment has been accumulating, and little is known about fungi biodegradation, especially in dry environments. Therefore, the research on plastic degradation technology is urgent. In this study, we demonstrated that Phanerochaete chrysosporium (P. chrysposporium), a typical species of white rot fungi, could react as a highly efficient biodegrader of polylactic acid (PLA), and 34.35 % of PLA degradation was obtained during 35-day incubation. A similar mass loss of 19.71 % could be achieved for polystyrene (PS) degradation. Here, we presented the visualization of the plastic deterioration process and their negative reciprocal on cell development, which may be caused by the challenge of using PS as a substrate. The RNA-seq analysis indicated that adaptations in energy metabolism and cellular defense were downregulated in the PS group, while lipid synthesis was upregulated in the PLA-treated group. Possible differentially expressed genes (DEG) of plastic degradation, such as hydrophobic proteins, lignin peroxidase (LiP), manganese peroxidase (MnP) and laccase (Lac), Cytochrome P450 (CYP450), and genes involved in styrene or benzoic acid degradation pathways have been recorded, and we proposed a PS degradation pathway.
Collapse
Affiliation(s)
- Feiyan Wu
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| | - Zhi Guo
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China.
| | - Kangping Cui
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| | - Dazhuang Dong
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| | - Xue Yang
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| | - Jie Li
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| | - Zhangzhen Wu
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| | - Lele Li
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| | - Yaodan Dai
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| | - Tao Pan
- School of Resources and Environmental Engineering, Hefei University of Technology, Hefei 230009, China; Anhui Engineering Research Center of Industrial Wastewater Treatment and Resource Recovery, Hefei University of Technology, Hefei 230009, China
| |
Collapse
|
13
|
Relationship between failure strain, molecular weight, and chain extensibility in biodegradable polymers. J Mech Behav Biomed Mater 2023; 139:105663. [PMID: 36657195 DOI: 10.1016/j.jmbbm.2023.105663] [Citation(s) in RCA: 1] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 10/03/2022] [Revised: 01/02/2023] [Accepted: 01/05/2023] [Indexed: 01/07/2023]
Abstract
Prior to degradation, biocompatible polymers exhibit ductile behaviour and yield stress offers a suitable design approach. However, as degradation proceeds the material transitions to a brittle failure mode, suggesting a more conservative design approach is necessary. Here, we predict the evolving ductility of biodegrading polymers, concentrating on the relationship between molecular weight and failure strain, εf, in poly (lactic acid). Several datasets are chosen from literature to explore the relationship, with an overview of the experimental techniques provided. Failure criteria are proposed and examined alongside these datasets: the first assumes εf is related to the finite chain extensibility of an average chain; the second introduces an exponential empirical trend; the third proposes a modified extensibility criterion (based on the first criterion) that considers the entire molecular weight distribution; and the fourth offers an alternative to the third by considering the effect of chain scissions. Combining the failure criteria with a previously introduced time-dependent kinetic scission model provides results as a function of degradation duration. The predictions obtained can offer insight into material failure, particularly at advanced stages of degradation.
Collapse
|
14
|
Lykins WR, Bernards DA, Schlesinger EB, Wisniewski K, Desai TA. Tuning polycaprolactone degradation for long acting implantables. POLYMER 2022. [DOI: 10.1016/j.polymer.2022.125473] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/09/2022]
|
15
|
Kivijärvi T, Øyvind Goksøyr, Yassin MA, Jain S, Yamada S, Morales-López A, Mustafa K, Finne-Wistrand A. Hybrid material based on hyaluronan hydrogels and poly(l-lactide-co-1,3-trimethylene carbonate) scaffolds toward a cell-instructive microenvironment with long-term in vivo degradability. Mater Today Bio 2022; 17:100483. [DOI: 10.1016/j.mtbio.2022.100483] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 08/16/2022] [Revised: 10/14/2022] [Accepted: 10/29/2022] [Indexed: 11/16/2022] Open
|
16
|
Polidar M, Metzsch-Zilligen E, Pfaendner R. Controlled and Accelerated Hydrolysis of Polylactide (PLA) through Pentaerythritol Phosphites with Acid Scavengers. Polymers (Basel) 2022; 14:polym14194237. [PMID: 36236186 PMCID: PMC9573666 DOI: 10.3390/polym14194237] [Citation(s) in RCA: 7] [Impact Index Per Article: 3.5] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 06/24/2022] [Revised: 07/19/2022] [Accepted: 07/21/2022] [Indexed: 11/16/2022] Open
Abstract
This study provides insight into the accelerated hydrolysis of polyester PLA through the addition of phosphites based on pentaerythritol. To control hydrolysis and ensure processing stability, different types of phosphites and combinations of phosphites with acid scavengers were studied. Therefore, commercially available PLA was compounded with selected additives on a twin-screw extruder, and hydrolysis experiments were performed at 23 °C, 35 °C and 58 °C in deionized water. Hydrolysis of PLA was evaluated by the melt volume rate (MVR) and size-exclusion chromatography (SEC). For example, after 4 days of water storage at 58 °C, the number average molecular weight of the PLA comparison sample was reduced by 31.3%, whereas PLA compounded with 0.8% phosphite P1 had a 57.7% lower molecular weight. The results are in good agreement with the expected and tested stability against hydrolysis of the investigated phosphite structures. 31P-NMR spectroscopy was utilized to elucidate the hydrolysis of phosphites in the presence of lactic acid. With the addition of phosphites based on pentaerythritol, the hydrolysis rate can be enhanced, and faster biodegradation behavior of biodegradable polyesters is expected. Accelerated biodegradation is beneficial for reducing the residence time of polymers in composting facilities or during home composting and as litter or microplastic residues.
Collapse
|
17
|
Hill A, Ronan W. A kinetic scission model for molecular weight evolution in bioresorbable polymers. POLYM ENG SCI 2022. [DOI: 10.1002/pen.26131] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/05/2022]
Affiliation(s)
- Aoife Hill
- Biomechanics Research Centre, Biomedical Engineering, School of Engineering University of Galway Galway Ireland
| | - William Ronan
- Biomechanics Research Centre, Biomedical Engineering, School of Engineering University of Galway Galway Ireland
| |
Collapse
|
18
|
|
19
|
Xu PY, Liu TY, Huang D, Zhen ZC, Lu B, Li X, Zheng WZ, Wang GX, Ji JH. Degradation performances of CL-modified PBSCL copolyesters in different environments. Eur Polym J 2022. [DOI: 10.1016/j.eurpolymj.2022.111322] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/04/2022]
|
20
|
Wei P, Li L, Wang L, Yan J, Zeng N, Li L, Sun N, Bai L, Li H, Zhang Y. Synthesis and properties of high performance biobased liquid crystal copolyesters toward load-bearing bone repair application. Eur Polym J 2022. [DOI: 10.1016/j.eurpolymj.2022.111278] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/04/2022]
|
21
|
Grivet-Brancot A, Boffito M, Ciardelli G. Use of Polyesters in Fused Deposition Modeling for Biomedical Applications. Macromol Biosci 2022; 22:e2200039. [PMID: 35488769 DOI: 10.1002/mabi.202200039] [Citation(s) in RCA: 1] [Impact Index Per Article: 0.5] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 01/29/2022] [Revised: 04/11/2022] [Indexed: 11/09/2022]
Abstract
In recent years, 3D printing techniques experienced a growing interest in several sectors, including the biomedical one. Their main advantage resides in the possibility to obtain complex and personalized structures in a cost-effective way impossible to achieve with traditional production methods. This is especially true for Fused Deposition Modeling (FDM), one of the most diffused 3D printing methods. The easy customization of the final products' geometry, composition and physico-chemical properties is particularly interesting for the increasingly personalized approach adopted in modern medicine. Thermoplastic polymers are the preferred choice for FDM applications, and a wide selection of biocompatible and biodegradable materials is available to this aim. Moreover, these polymers can also be easily modified before and after printing to better suit the body environment and the mechanical properties of biological tissues. This review focuses on the use of thermoplastic aliphatic polyesters for FDM applications in the biomedical field. In detail, the use of poly(ε-caprolactone), poly(lactic acid), poly(lactic-co-glycolic acid), poly(hydroxyalkanoate)s, thermo-plastic poly(ester urethane)s and their blends has been thoroughly surveyed, with particular attention to their main features, applicability and workability. The state-of-the-art is presented and current challenges in integrating the additive manufacturing technology in the medical practice are discussed. This article is protected by copyright. All rights reserved.
Collapse
Affiliation(s)
- Arianna Grivet-Brancot
- Department of Mechanical and Aerospace Engineering, Politecnico di Torino, Corso Duca degli Abruzzi, 24, Torino, 10129, Italy.,Department of Surgical Sciences, Università di Torino, Corso Dogliotti 14, Torino, 10126, Italy
| | - Monica Boffito
- Department of Mechanical and Aerospace Engineering, Politecnico di Torino, Corso Duca degli Abruzzi, 24, Torino, 10129, Italy
| | - Gianluca Ciardelli
- Department of Mechanical and Aerospace Engineering, Politecnico di Torino, Corso Duca degli Abruzzi, 24, Torino, 10129, Italy
| |
Collapse
|
22
|
Bozkaya O, Arat E, Gün Gök Z, Yiğitoğlu M, Vargel İ. Production and characterization of hybrid nanofiber wound dressing containing Centella asiatica coated silver nanoparticles by mutual electrospinning method. Eur Polym J 2022. [DOI: 10.1016/j.eurpolymj.2022.111023] [Citation(s) in RCA: 6] [Impact Index Per Article: 3.0] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 12/20/2022]
|
23
|
Ivanova TA, Chumakova NA, Golubeva EN, Mel’nikov MY. Kinetics of Release of a Bifunctional 2,2,5,5-Tetramethyl-4-Phenyl-3-Imidazoline-1-Oxyl-3-Oxide Probe from Poly-D,L-Lactide Films Formed Using Supercritical Carbon Dioxide. RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY B 2022. [DOI: 10.1134/s1990793121080066] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 11/23/2022]
|
24
|
Chen H, Shi Q, Shui H, Wang P, Chen Q, Li Z. Degradation of 3D-Printed Porous Polylactic Acid Scaffolds Under Mechanical Stimulus. Front Bioeng Biotechnol 2021; 9:691834. [PMID: 34765591 PMCID: PMC8576397 DOI: 10.3389/fbioe.2021.691834] [Citation(s) in RCA: 3] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 04/07/2021] [Accepted: 09/14/2021] [Indexed: 11/13/2022] Open
Abstract
Polylactic acid (PLA) is a biodegradable polymer commonly used as a scaffold material to repair tissue defects, and its degradation is associated with mechanical stimulus. In this study, the effect of mechanical stimulus on the degradation of 3D-printed PLA scaffolds was investigated by in vitro experiments and an author-developed numerical model. Forty-five samples with porosity 64.8% were printed to carry out the degradation experiment within 90 days. Statistical analyses of the mass, volume fraction, Young’s modulus, and number average molecular weight were made, and the in vitro experiments were further used to verify the proposed numerical model of the scaffold degradation. The results indicated that the mechanical stimulus accelerated the degradation of the PLA scaffold, and the higher mechanical stimulus led to a faster degradation of the scaffolds at the late stage of the degradation process. In addition, the Young’s modulus and the normalized number average molecular weight of the PLA scaffolds between the experiments and the numerical simulations were comparable, especially for the number average molecular weight. The present study could be helpful in the design of the biodegradable PLA scaffolds.
Collapse
Affiliation(s)
- Heming Chen
- School of Biological Science and Medical Engineering, Southeast University, Nanjing, China
| | - Quan Shi
- School of Biological Science and Medical Engineering, Southeast University, Nanjing, China
| | - Hengtao Shui
- School of Biological Science and Medical Engineering, Southeast University, Nanjing, China
| | - Peng Wang
- State Key Laboratory of Pharmaceutical Biotechnology, Department of Sports Medicine and Adult Reconstructive Surgery, Nanjing Drum Tower Hospital, The Affiliated Hospital of Nanjing University Medical School, Nanjing, China
| | - Qiang Chen
- School of Biological Science and Medical Engineering, Southeast University, Nanjing, China
| | - Zhiyong Li
- School of Biological Science and Medical Engineering, Southeast University, Nanjing, China.,School of Mechanical, Medical and Process Engineering, Queensland University of Technology, Brisbane, QLD, Australia
| |
Collapse
|
25
|
Simulate SubQ: The Methods and the Media. J Pharm Sci 2021; 112:1492-1508. [PMID: 34728176 DOI: 10.1016/j.xphs.2021.10.031] [Citation(s) in RCA: 3] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 08/16/2021] [Revised: 10/25/2021] [Accepted: 10/26/2021] [Indexed: 11/21/2022]
Abstract
For decades, there has been a growing interest in injectable subcutaneous formulations to improve the absorption of drugs into the systemic circulation and to prolong their release over a longer period. However, fluctuations in the blood plasma levels together with bioavailability issues often limit their clinical success. This warrants a closer look at the performance of long-acting depots, for example, and their dependence on the complex interplay between the dosage form and the physiological microenvironment. For this, biopredictive performance testing is used for a thorough understanding of the biophysical processes affecting the absorption of compounds from the injection site in vivo and their simulation in vitro. In the present work, we discuss in vitro methodologies including methods and media developed for the subcutaneous route of administration on the background of the most relevant absorption mechanisms. Also, we highlight some important knowledge gaps and shortcomings of the existing methodologies to provide the reader with a better understanding of the scientific evidence underlying these models.
Collapse
|
26
|
Zhang T, Chen H, Guo X, Yu Y, Wulamu A. A structure dynamic interaction multiscale method for degradation modeling of bioresorbable polyesters. Polym Degrad Stab 2021. [DOI: 10.1016/j.polymdegradstab.2021.109704] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 10/20/2022]
|
27
|
|
28
|
Bufton J, Jung S, Evans JC, Bao Z, Aguiar D, Allen C. Cross-linked valerolactone copolymer implants with tailorable biodegradation, loading and in vitro release of paclitaxel. Eur J Pharm Sci 2021; 162:105808. [DOI: 10.1016/j.ejps.2021.105808] [Citation(s) in RCA: 2] [Impact Index Per Article: 0.7] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 11/09/2020] [Revised: 02/18/2021] [Accepted: 03/11/2021] [Indexed: 12/20/2022]
|
29
|
Ali AF, Ahmed MM, El-Kady AM, Abd El-Hady BM, Ibrahim AM. Synthesis of Gelatin-Agarose Scaffold for Controlled Antibiotic Delivery and its Modification by Glass Nanoparticles Addition as a Potential Osteomyelitis Treatment. SILICON 2021; 13:2011-2028. [DOI: 10.1007/s12633-020-00576-1] [Citation(s) in RCA: 4] [Impact Index Per Article: 1.3] [Reference Citation Analysis] [Track Full Text] [Subscribe] [Scholar Register] [Received: 02/08/2020] [Accepted: 06/26/2020] [Indexed: 09/02/2023]
|
30
|
Naddeo M, Sorrentino A, Pappalardo D. Thermo-Rheological and Shape Memory Properties of Block and Random Copolymers of Lactide and ε-Caprolactone. Polymers (Basel) 2021; 13:627. [PMID: 33669678 PMCID: PMC7922056 DOI: 10.3390/polym13040627] [Citation(s) in RCA: 9] [Impact Index Per Article: 3.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 01/19/2021] [Revised: 02/11/2021] [Accepted: 02/16/2021] [Indexed: 12/23/2022] Open
Abstract
Biodegradable block and random copolymers have attracted numerous research interests in different areas, due to their capability to provide a broad range of properties. In this paper, an efficient strategy has been reported for preparing biodegradable PCL-PLA copolymers with improved thermal, mechanical and rheological properties. Two block-copolymers are synthesized by sequential addition of the cyclic esters lactide (L-LA or D,L-LA) and ε-caprolactone (CL) in presence of a dimethyl(salicylaldiminato)aluminium compound. The random copolymer of L-LA and CL was synthetized by using the same catalyst. Chain structure, molar mass, thermal, rheological and mechanical properties are characterized by NMR, SEC, TGA, DSC, Rheometry and DMTA. Experimental results show that by changing the stereochemistry and monomer distribution of the copolymers it is possible to obtain a variety of properties. Promising shape-memory properties are also observed in the di-block copolymers characterized by the co-crystallization of CL and L-LA segments. These materials show great potential to substitute oil-based polymers for packaging, electronics, and medicine applications.
Collapse
Affiliation(s)
- Marco Naddeo
- Dipartimento di Scienze e Tecnologie, Università del Sannio, via de Sanctis snc, 82100 Benevento, Italy;
| | - Andrea Sorrentino
- Institute for Polymers, Composites and Biomaterials (IPCB-CNR), P.le E Fermi, 1, 80055 Portici, Italy
| | - Daniela Pappalardo
- Dipartimento di Scienze e Tecnologie, Università del Sannio, via de Sanctis snc, 82100 Benevento, Italy;
| |
Collapse
|
31
|
Ekinci A, Gleadall A, Johnson AA, Li L, Han X. Mechanical and hydrolytic properties of thin polylactic acid films by fused filament fabrication. J Mech Behav Biomed Mater 2020; 114:104217. [PMID: 33246876 DOI: 10.1016/j.jmbbm.2020.104217] [Citation(s) in RCA: 8] [Impact Index Per Article: 2.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 06/23/2020] [Revised: 10/26/2020] [Accepted: 11/15/2020] [Indexed: 01/14/2023]
Abstract
Thin polymeric films are widely used as medical applications such as cell culture, stent, drug delivery and mechanical fixation. One of the most commonly used materials is polylactic acid (PLA) - a material, which is non-toxic, biodegradable and biocompatible. Fused filament fabrication (FFF) is a preferable additive manufacturing technique to manufacture polymers, where PLA is one of the most common materials. FFF is a promising technique for customised biomedical applications due to its relatively low cost and geometrical flexibility where biomedical applications are patient tailored. This study is the first to consider FFF monolayered thin films of PLA in terms of mechanical and hydrolytic properties at 37 °C in vitro degradation. Throughout degradation, the reduction in mechanical properties was examined by analysing molecular weight and thermal properties. FFF monolayered PLA underwent autocatalytic bulk degradation with no proof of significant mass loss. Young's modulus, ultimate tensile strength and molecular weight reduced by approximately 60%, 86%, and 80% after 280 days, respectively, while the degree of crystallinity increased by 143% in comparison to benchmark thin films at day 0. It was found that the decrease in mechanical properties was more sensitive to the increase in crystallinity in the early stage of the degradation, while the molecular weight was more dominant in the late stage of the degradation. This study provides practical information in terms of mechanical properties to support medical device designers in a range of potential end-use biomedical applications to achieve safe functional products over the required degradation lifetime.
Collapse
Affiliation(s)
- Alper Ekinci
- Wolfson School of Mechanical, Electrical and Manufacturing Engineering, Loughborough University, Loughborough, LE11 3TU, UK
| | - Andy Gleadall
- Wolfson School of Mechanical, Electrical and Manufacturing Engineering, Loughborough University, Loughborough, LE11 3TU, UK
| | - Andrew A Johnson
- School of Design & Creative Arts, Loughborough University, Loughborough, LE11 3TU, UK
| | - Ling Li
- State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Hunan University, 410082, China
| | - Xiaoxiao Han
- State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Hunan University, 410082, China.
| |
Collapse
|
32
|
Guo C, Dou J. Degradation Simulation of Poly Lactic Acid in Vitro Using the Genetic Algorithm. ACS Biomater Sci Eng 2020; 6:6126-6137. [PMID: 33449676 DOI: 10.1021/acsbiomaterials.0c01325] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/30/2022]
Abstract
Computer simulation using a degradation model is the most effective method to investigate the degradation behaviors of poly lactic acid (PLA). Various kinetic parameters are introduced into numerous degradation models to achieve the best simulation result. Nevertheless, massive possibilities of different parameter combinations limit the application of the enumeration algorithm, while the nonlinear relationship between the kinetic parameters and the degradation behaviors of PLA indicates that the ordinary parameter search algorithms cannot do well in the parameter optimization. A genetic algorithm (GA) with a small population size is proposed and utilized to optimize the kinetic parameters of the cellular automaton (CA) simulation in the present work. The optimal result indicates that the presented GA can realize the parameter optimization of the CA degradation model. The elitist tournament selection operation can speed up the optimization process. The algorithm can be executed as a single-stage algorithm alone or applied as a multistage algorithm according to various solution objects and corresponding fitness functions. Moreover, the algorithm can be hybridized with other traditional search methods such as binary search or local enumeration search to achieve a balance between accuracy and search speed.
Collapse
Affiliation(s)
- Chao Guo
- School of Materials Science and Engineering and Jiangsu Key Laboratory of Advanced Metallic Materials, Southeast University, Nanjing 211189, China
| | - Jian Dou
- Institute of Botany, Jiangsu Province and Chinese Academy of Sciences, Nanjing 210014, China
| |
Collapse
|
33
|
Strength modeling for degradation of bioresorbable polyesters based on phase image pattern recognition. Polym Degrad Stab 2020. [DOI: 10.1016/j.polymdegradstab.2020.109291] [Citation(s) in RCA: 2] [Impact Index Per Article: 0.5] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/22/2022]
|
34
|
Song C, Zhang J, Cen L, Xi Z, Zhao L, Yuan W. Modeling Strategies for the Degradation Behavior of Porous Polyester Materials Based on Their Key Structural Features. Ind Eng Chem Res 2020. [DOI: 10.1021/acs.iecr.0c02694] [Citation(s) in RCA: 2] [Impact Index Per Article: 0.5] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/30/2022]
Affiliation(s)
- Chaobo Song
- State Key Laboratory of Chemical Engineering, School of Chemical Engineering, East China University of Science and Technology, Shanghai 200237, China
| | - Jiapeng Zhang
- State Key Laboratory of Chemical Engineering, School of Chemical Engineering, East China University of Science and Technology, Shanghai 200237, China
| | - Lian Cen
- State Key Laboratory of Chemical Engineering, School of Chemical Engineering, East China University of Science and Technology, Shanghai 200237, China
| | - Zhenhao Xi
- State Key Laboratory of Chemical Engineering, School of Chemical Engineering, East China University of Science and Technology, Shanghai 200237, China
| | - Ling Zhao
- State Key Laboratory of Chemical Engineering, School of Chemical Engineering, East China University of Science and Technology, Shanghai 200237, China
- College of Chemistry and Chemical Engineering, Xinjiang University, Urumqi 830046, China
| | - Weikang Yuan
- State Key Laboratory of Chemical Engineering, School of Chemical Engineering, East China University of Science and Technology, Shanghai 200237, China
| |
Collapse
|
35
|
Rahman M, Dutta NK, Roy Choudhury N. Magnesium Alloys With Tunable Interfaces as Bone Implant Materials. Front Bioeng Biotechnol 2020; 8:564. [PMID: 32587850 PMCID: PMC7297987 DOI: 10.3389/fbioe.2020.00564] [Citation(s) in RCA: 34] [Impact Index Per Article: 8.5] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 02/05/2020] [Accepted: 05/11/2020] [Indexed: 12/20/2022] Open
Abstract
Magnesium (Mg) based biodegradable materials are a new generation orthopedic implant materials that are intended to possess same mechanical properties as that of bone. Mg alloys are considered as promising substitutes to permanent implants due to their biodegradability in the physiological environment. However, rapid corrosion rate is one of the major constraints of using Mg alloys in clinical applications in spite of their excellent biocompatibility. Approaches to overcome the limitations include the selection of adequate alloying elements, proper surface treatment, surface modification with coating to control the degradation rate. This review focuses on current advances on surface engineering of Mg based biomaterials for biomedical applications. The review begins with a description of corrosion mechanism of Mg alloy, the requirement for appropriate surface functionalization/coatings, their structure-property-performance relationship, and suitability for biomedical applications. The control of physico-chemical properties such as wettability, surface morphology, surface chemistry, and surface functional groups of the coating tailored by various approaches forms the pivotal part of the review. Chemical surface treatment offers initial protection from corrosion and inorganic coating like hydroxyapatite (HA) improves the biocompatibility of the substrate. Considering the demand of ideal implant materials, multilayer hybrid coatings on Mg alloy in combination with chemical pretreatment or inorganic HA coating, and protein-based polymer coating could be a promising technique to improve corrosion resistance and promote biocompatibility of Mg-based alloys.
Collapse
Affiliation(s)
| | | | - Namita Roy Choudhury
- Chemical and Environmental Engineering, School of Engineering, RMIT University, Melbourne, VIC, Australia
| |
Collapse
|
36
|
Pietrzykowska E, Romelczyk-Baishya B, Wojnarowicz J, Sokolova M, Szlazak K, Swieszkowski W, Locs J, Lojkowski W. Preparation of a Ceramic Matrix Composite Made of Hydroxyapatite Nanoparticles and Polylactic Acid by Consolidation of Composite Granules. NANOMATERIALS 2020; 10:nano10061060. [PMID: 32486301 PMCID: PMC7352493 DOI: 10.3390/nano10061060] [Citation(s) in RCA: 4] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Subscribe] [Scholar Register] [Received: 03/31/2020] [Revised: 05/15/2020] [Accepted: 05/15/2020] [Indexed: 12/20/2022]
Abstract
Composites made of a biodegradable polymer, e.g., polylactic acid (PLA) and hydroxyapatite nanoparticles (HAP NPs) are promising orthopedic materials. There is a particular need for biodegradable hybrid nanocomposites with strong mechanical properties. However, obtaining such composites is challenging, since nanoparticles tend to agglomerate, and it is difficult to achieve good bonding between the hydrophilic ceramic and the hydrophobic polymer. This paper describes a two-step technology for obtaining a ceramic matrix composite. The first step is the preparation of composite granules. The granules are obtained by infiltration of porous granules of HAP NPs with PLA through high-pressure infiltration. The homogeneous ceramic-polymer granules are 80 μm in diameter, and the composite granules are 80 wt% HAP NPs. The second step is consolidation of the granules using high pressure. This is performed in three variants: Uniaxial pressing with the pressure of up to 1000 MPa at room temperature, warm isostatic compaction (75 MPa at 155 °C), and a combination of the two methods. The combined methods result in the highest densification (99%) and strongest mechanical properties; the compressive strength is 374 MPa. The structure of the ceramic matrix composite is homogeneous. Good adhesion between the inorganic and the organic component is observable using scanning electron microscopy.
Collapse
Affiliation(s)
- Elzbieta Pietrzykowska
- Institute of High Pressure Physics, Polish Academy of Science, Sokolowska 29/37, 01-142 Warsaw, Poland; (J.W.); (W.L.)
- Faculty of Materials Science and Engineering, Warsaw University of Technology, Woloska 141, 02-507 Warsaw, Poland; (B.R.-B.); (K.S.); (W.S.)
- Correspondence: ; Tel.: +48-228-760-429
| | - Barbara Romelczyk-Baishya
- Faculty of Materials Science and Engineering, Warsaw University of Technology, Woloska 141, 02-507 Warsaw, Poland; (B.R.-B.); (K.S.); (W.S.)
| | - Jacek Wojnarowicz
- Institute of High Pressure Physics, Polish Academy of Science, Sokolowska 29/37, 01-142 Warsaw, Poland; (J.W.); (W.L.)
| | - Marina Sokolova
- Rudolfs Cimdins Riga Biomaterials Innovations and Development Centre of RTU, Institute of General Chemical Engineering, Faculty of Materials Science and Applied Chemistry, Riga Technical University, Pulka Street 3, LV-1007 Riga, Latvia; (M.S.); (J.L.)
| | - Karol Szlazak
- Faculty of Materials Science and Engineering, Warsaw University of Technology, Woloska 141, 02-507 Warsaw, Poland; (B.R.-B.); (K.S.); (W.S.)
| | - Wojciech Swieszkowski
- Faculty of Materials Science and Engineering, Warsaw University of Technology, Woloska 141, 02-507 Warsaw, Poland; (B.R.-B.); (K.S.); (W.S.)
| | - Janis Locs
- Rudolfs Cimdins Riga Biomaterials Innovations and Development Centre of RTU, Institute of General Chemical Engineering, Faculty of Materials Science and Applied Chemistry, Riga Technical University, Pulka Street 3, LV-1007 Riga, Latvia; (M.S.); (J.L.)
| | - Witold Lojkowski
- Institute of High Pressure Physics, Polish Academy of Science, Sokolowska 29/37, 01-142 Warsaw, Poland; (J.W.); (W.L.)
| |
Collapse
|
37
|
Golubeva EN, Chumakova NA. Spin Probe Method for Diagnostics of Polyester Porous Matrixes Formed in Supercritical Carbon Dioxide (Review). RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY B 2020. [DOI: 10.1134/s1990793119070078] [Citation(s) in RCA: 3] [Impact Index Per Article: 0.8] [Reference Citation Analysis] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 01/22/2023]
|
38
|
Ivanova TA, Chumakova NA, Golubeva EN, Lunin VV. Kinetics of Release of the TEMPONE Nitroxyl Radical from Poly-D,L-Lactide Foamed in the Supercritical Carbon Dioxide Medium. RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY B 2020. [DOI: 10.1134/s199079311907025x] [Citation(s) in RCA: 2] [Impact Index Per Article: 0.5] [Reference Citation Analysis] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 11/23/2022]
|
39
|
Ehrmann K, Potzmann P, Dworak C, Bergmeister H, Eilenberg M, Grasl C, Koch T, Schima H, Liska R, Baudis S. Hard Block Degradable Polycarbonate Urethanes: Promising Biomaterials for Electrospun Vascular Prostheses. Biomacromolecules 2020; 21:376-387. [PMID: 31718163 DOI: 10.1021/acs.biomac.9b01255] [Citation(s) in RCA: 13] [Impact Index Per Article: 3.3] [Reference Citation Analysis] [Abstract] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 12/17/2022]
Abstract
We report biodegradable thermoplastic polyurethanes for soft tissue engineering applications, where frequently used carboxylic acid ester degradation motifs were substituted with carbonate moieties to achieve superior degradation properties. While the use of carbonates in soft blocks has been reported, their use in hard blocks of thermoplastic polyurethanes is unprecedented. Soft blocks consist of poly(hexamethylene carbonate), and hard blocks combine hexamethylene diisocyanate with the newly synthesized cleavable carbonate chain extender bis(3-hydroxypropylene)carbonate (BHPC), mimicking the motif of poly(trimethylene carbonate) with highly regarded degradation properties. Simultaneously, the mechanical benefits of segmented polyurethanes are exploited. A lower hard block concentration in BHPC-based polymers was more suitable for vascular grafts. Nonacidic degradation products and hard block dependent degradation rates were found. Implantation of BHPC-based electrospun degradable vascular prostheses in a small animal model revealed high patency rates and no signs of aneurysm formations. Specific vascular graft remodeling and only minimal signs of inflammatory reactions were observed.
Collapse
Affiliation(s)
- Katharina Ehrmann
- Institute of Applied Synthetic Chemistry, Division of Macromolecular Chemistry , TU Wien , Getreidemarkt 9/163 MC , 1060 Vienna , Austria.,Division of Biomedical Research , Medical University of Vienna , Währinger Gürtel 18-20 , 1090 Vienna , Austria.,Austrian Cluster for Tissue Regeneration , 1200 Vienna , Austria
| | - Paul Potzmann
- Institute of Applied Synthetic Chemistry, Division of Macromolecular Chemistry , TU Wien , Getreidemarkt 9/163 MC , 1060 Vienna , Austria.,Austrian Cluster for Tissue Regeneration , 1200 Vienna , Austria
| | - Claudia Dworak
- Institute of Applied Synthetic Chemistry, Division of Macromolecular Chemistry , TU Wien , Getreidemarkt 9/163 MC , 1060 Vienna , Austria.,Austrian Cluster for Tissue Regeneration , 1200 Vienna , Austria
| | - Helga Bergmeister
- Division of Biomedical Research , Medical University of Vienna , Währinger Gürtel 18-20 , 1090 Vienna , Austria.,Ludwig Boltzmann Institute for Cardiovascular Research , Währinger Gürtel 18-20 , 1090 Vienna , Austria.,Austrian Cluster for Tissue Regeneration , 1200 Vienna , Austria
| | - Magdalena Eilenberg
- Division of Biomedical Research , Medical University of Vienna , Währinger Gürtel 18-20 , 1090 Vienna , Austria.,Department of Surgery , Medical University of Vienna , Währinger Gürtel 18-20 , 1090 Vienna , Austria
| | - Christian Grasl
- Ludwig Boltzmann Institute for Cardiovascular Research , Währinger Gürtel 18-20 , 1090 Vienna , Austria.,Center for Medical Physics and Biomedical Engineering , Medical University of Vienna , Währinger Gürtel 18-20 , 1090 Vienna , Austria
| | - Thomas Koch
- Institute of Materials Science and Technology , TU Wien , Getreidemarkt 9/308 , 1060 Vienna , Austria
| | - Heinrich Schima
- Ludwig Boltzmann Institute for Cardiovascular Research , Währinger Gürtel 18-20 , 1090 Vienna , Austria.,Center for Medical Physics and Biomedical Engineering , Medical University of Vienna , Währinger Gürtel 18-20 , 1090 Vienna , Austria
| | - Robert Liska
- Institute of Applied Synthetic Chemistry, Division of Macromolecular Chemistry , TU Wien , Getreidemarkt 9/163 MC , 1060 Vienna , Austria.,Austrian Cluster for Tissue Regeneration , 1200 Vienna , Austria
| | - Stefan Baudis
- Institute of Applied Synthetic Chemistry, Division of Macromolecular Chemistry , TU Wien , Getreidemarkt 9/163 MC , 1060 Vienna , Austria.,Austrian Cluster for Tissue Regeneration , 1200 Vienna , Austria
| |
Collapse
|
40
|
Walejewska E, Idaszek J, Heljak M, Chlanda A, Choinska E, Hasirci V, Swieszkowski W. The effect of introduction of filament shift on degradation behaviour of PLGA- and PLCL-based scaffolds fabricated via additive manufacturing. Polym Degrad Stab 2020. [DOI: 10.1016/j.polymdegradstab.2019.109030] [Citation(s) in RCA: 3] [Impact Index Per Article: 0.8] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 02/08/2023]
|
41
|
|
42
|
Larrañaga A, Lizundia E. A review on the thermomechanical properties and biodegradation behaviour of polyesters. Eur Polym J 2019. [DOI: 10.1016/j.eurpolymj.2019.109296] [Citation(s) in RCA: 67] [Impact Index Per Article: 13.4] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 12/31/2022]
|
43
|
Oosterbeek RN, Kwon KA, Duffy P, McMahon S, Zhang XC, Best SM, Cameron RE. Tuning structural relaxations, mechanical properties, and degradation timescale of PLLA during hydrolytic degradation by blending with PLCL-PEG. Polym Degrad Stab 2019. [DOI: 10.1016/j.polymdegradstab.2019.109015] [Citation(s) in RCA: 11] [Impact Index Per Article: 2.2] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 02/08/2023]
|
44
|
Ficek K, Rajca J, Stolarz M, Stodolak-Zych E, Wieczorek J, Muzalewska M, Wyleżoł M, Wróbel Z, Binkowski M, Błażewicz S. Bioresorbable Stent in Anterior Cruciate Ligament Reconstruction. Polymers (Basel) 2019; 11:polym11121961. [PMID: 31795412 PMCID: PMC6960761 DOI: 10.3390/polym11121961] [Citation(s) in RCA: 11] [Impact Index Per Article: 2.2] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 10/18/2019] [Revised: 11/19/2019] [Accepted: 11/25/2019] [Indexed: 11/16/2022] Open
Abstract
The exact causes of failure of anterior cruciate ligament (ACL) reconstruction are still unknown. A key to successful ACL reconstruction is the prevention of bone tunnel enlargement (BTE). In this study, a new strategy to improve the outcome of ACL reconstruction was analyzed using a bioresorbable polylactide (PLA) stent as a catalyst for the healing process. The study included 24 sheep with 12 months of age. The animals were randomized to the PLA group (n = 16) and control group (n = 8), subjected to the ACL reconstruction with and without the implantation of the PLA tube, respectively. The sheep were sacrificed 6 or 12 weeks post-procedure, and their knee joints were evaluated by X-ray microcomputed tomography with a 50 μm resolution. While the analysis of tibial and femoral tunnel diameters and volumes demonstrated the presence of BTE in both groups, the enlargement was less evident in the PLA group. Also, the microstructural parameters of the bone adjacent to the tunnels tended to be better in the PLA group. This suggested that the implantation of a bioresorbable PLA tube might facilitate osteointegration of the tendon graft after the ACL reconstruction. The beneficial effects of the stent were likely associated with osteogenic and osteoconductive properties of polylactide.
Collapse
Affiliation(s)
- Krzysztof Ficek
- Department of Science, Innovation and Development, Galen-Orthopaedics, 43-150 Bierun, Poland; (K.F.); (M.S.)
- Department of Physiotherapy, Academy of Physical Education, 40-065 Katowice, Poland
| | - Jolanta Rajca
- Department of Science, Innovation and Development, Galen-Orthopaedics, 43-150 Bierun, Poland; (K.F.); (M.S.)
- Correspondence:
| | - Mateusz Stolarz
- Department of Science, Innovation and Development, Galen-Orthopaedics, 43-150 Bierun, Poland; (K.F.); (M.S.)
- Department of Orthopedics and Traumatology, City Hospital in Zabrze, 41-803 Zabrze, Poland
| | - Ewa Stodolak-Zych
- Department of Biomaterials and Composites, Faculty of Materials Science and Ceramics, AGH University of Science and Technology, 30-059 Krakow, Poland; (E.S.-Z.); (S.B.)
| | - Jarosław Wieczorek
- University Center of Veterinary Medicine UJ-UR, University of Agriculture in Krakow, 30-059 Krakow, Poland;
| | - Małgorzata Muzalewska
- Institute of Fundamentals of Machinery Design, Faculty of Mechanical Engineering, Silesian University of Technology, 44-100 Gliwice, Poland; (M.M.); (M.W.)
| | - Marek Wyleżoł
- Institute of Fundamentals of Machinery Design, Faculty of Mechanical Engineering, Silesian University of Technology, 44-100 Gliwice, Poland; (M.M.); (M.W.)
| | - Zygmunt Wróbel
- Institute of Biomedical Engineering, Faculty of Science and Technology, University of Silesia, 41-205 Sosnowiec, Poland;
| | - Marcin Binkowski
- X-ray Microtomography Lab, Department of Computer Biomedical Systems, Institute of Computer Science, Faculty of Computer and Materials Science, University of Silesia, 41-200 Sosnowiec, Poland;
| | - Stanisław Błażewicz
- Department of Biomaterials and Composites, Faculty of Materials Science and Ceramics, AGH University of Science and Technology, 30-059 Krakow, Poland; (E.S.-Z.); (S.B.)
| |
Collapse
|
45
|
Zhao R, Xu Z, Li B, Chen T, Mei N, Wang C, Zhou Z, You L, Wu C, Wang X, Tang S. A comparative study on agarose acetate and PDLLA scaffold for rabbit femur defect regeneration. ACTA ACUST UNITED AC 2019; 14:065007. [PMID: 31422950 DOI: 10.1088/1748-605x/ab3c1b] [Citation(s) in RCA: 1] [Impact Index Per Article: 0.2] [Reference Citation Analysis] [Abstract] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 01/01/2023]
Abstract
The development of degradable polymer scaffolds is a key issue in bone regeneration. Poly(D, L-lactide) (PDLLA) and its derivatives have usually been applied to the construction of degradable scaffolds, but these scaffolds had problems with acidic degradation products and quick loss of mechanic strength during the later degradation, which usually led to scaffold collapse and cavity formation because of the slower rate of bone regeneration. In the present paper, a polysaccharide derivative, agarose acetate (AGA), was synthesized and a novel porous AGA scaffold was successfully developed through a salt-leaching process. The AGA scaffold had over 90% porosity without swelling in water, and compared to collapse and acidic products of PDLLA scaffold during degradation, the AGA scaffold maintained a stable morphology and a nearly neutral pH value over 18 months' degradation in PBS. A bone mesenchymal stem cells (BMSCs) adhesion and proliferation experiment showed that more cells adhered to the AGA scaffold than to the PDLLA scaffold. A subcutaneous implant test showed that the AGA scaffold slowly degraded and did not cause an inflammatory response surrounding the implantation lesion site. AGA scaffold was implanted into femur defects in New Zealand white rabbits to test its in vivo performance. Results indicated that the AGA scaffold accelerated the process of bone regeneration compared to the PDLLA group and, with time, new bone was formed from the margin toward the center of the scaffolds, and the scaffold left in place retained its porous structure without collapsing. Meanwhile, the AGA scaffold showed a low degradation rate and kept its shape during the in vivo degradation compared to the PDLLA scaffold. This performance could have the benefit of integrated regenerative bone being formed instead of cavities due to the quickly degraded scaffold disappearing. These results demonstrate that the AGA scaffold has significant potential in bone regeneration applications.
Collapse
Affiliation(s)
- Ruifang Zhao
- Biomedical Engineering Institute, Jinan University, Guangzhou 510632 People's Republic of China
| | | | | | | | | | | | | | | | | | | | | |
Collapse
|
46
|
Shui H, Shi Q, Pugno NM, Chen Q, Li Z. Effect of mechanical stimulation on the degradation of poly(lactic acid) scaffolds with different designed structures. J Mech Behav Biomed Mater 2019; 96:324-333. [DOI: 10.1016/j.jmbbm.2019.04.028] [Citation(s) in RCA: 8] [Impact Index Per Article: 1.6] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 01/16/2019] [Revised: 04/12/2019] [Accepted: 04/16/2019] [Indexed: 12/23/2022]
|
47
|
Nowalk JA, Swisher JH, Meyer TY. Influence of Short-Range Scrambling of Monomer Order on the Hydrolysis Behaviors of Sequenced Degradable Polyesters. Macromolecules 2019. [DOI: 10.1021/acs.macromol.9b00480] [Citation(s) in RCA: 8] [Impact Index Per Article: 1.6] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 12/17/2022]
Affiliation(s)
- Jamie A. Nowalk
- Department of Chemistry, University of Pittsburgh, Pittsburgh, Pennsylvania 15260, United States
| | - Jordan H. Swisher
- Department of Chemistry, University of Pittsburgh, Pittsburgh, Pennsylvania 15260, United States
| | - Tara Y. Meyer
- Department of Chemistry, University of Pittsburgh, Pittsburgh, Pennsylvania 15260, United States
- McGowan Institute for Regenerative Medicine, University of Pittsburgh, Pittsburgh, Pennsylvania 15219, United States
| |
Collapse
|
48
|
Novel controllable degradation behavior and biocompatibility of segmented poly–ε–caprolactone in rats. Polym Degrad Stab 2019. [DOI: 10.1016/j.polymdegradstab.2019.01.012] [Citation(s) in RCA: 2] [Impact Index Per Article: 0.4] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/19/2022]
|
49
|
Fuoco T, Mathisen T, Finne-Wistrand A. Minimizing the time gap between service lifetime and complete resorption of degradable melt-spun multifilament fibers. Polym Degrad Stab 2019. [DOI: 10.1016/j.polymdegradstab.2019.02.026] [Citation(s) in RCA: 17] [Impact Index Per Article: 3.4] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/30/2022]
|
50
|
Dillon B, Doran P, Fuenmayor E, Healy AV, Gately NM, Major I, Lyons JG. The Influence of Low Shear Microbore Extrusion on the Properties of High Molecular Weight Poly(l-Lactic Acid) for Medical Tubing Applications. Polymers (Basel) 2019; 11:polym11040710. [PMID: 31003549 PMCID: PMC6523984 DOI: 10.3390/polym11040710] [Citation(s) in RCA: 8] [Impact Index Per Article: 1.6] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 01/28/2019] [Revised: 04/08/2019] [Accepted: 04/10/2019] [Indexed: 11/21/2022] Open
Abstract
Biodegradable polymers play a crucial role in the medical device field, with a broad range of applications such as suturing, drug delivery, tissue engineering, scaffolding, orthopaedics, and fixation devices. Poly-l-lactic acid (PLLA) is one of the most commonly used and investigated biodegradable polymers. The objective of this study was to determine the influence low shear microbore extrusion exerts on the properties of high molecular weight PLLA for medical tubing applications. Results showed that even at low shear rates there was a considerable reduction in molecular weight (Mn = 7–18%) during processing, with a further loss (Mn 11%) associated with resin drying. An increase in melt residence time from ~4 mins to ~6 mins, translated into a 12% greater reduction in molecular weight. The degradation mechanism was determined to be thermal and resulted in a ~22-fold increase in residual monomer. The differences in molecular weight between both batches had no effect on the materials thermal or morphological properties. However, it did affect its mechanical properties, with a significant impact on tensile strength and modulus. Interestingly there was no effect on the elongational proprieties of the tubing. There was also an observed temperature-dependence of mechanical properties below the glass transition temperature.
Collapse
Affiliation(s)
- Brian Dillon
- Materials Research Institute, Athlone Institute of Technology, Dublin Road, Bunnavally, Athlone and Co. Westmeath, Ireland.
| | - Patrick Doran
- Materials Research Institute, Athlone Institute of Technology, Dublin Road, Bunnavally, Athlone and Co. Westmeath, Ireland.
| | - Evert Fuenmayor
- Materials Research Institute, Athlone Institute of Technology, Dublin Road, Bunnavally, Athlone and Co. Westmeath, Ireland.
| | - Andrew V Healy
- Materials Research Institute, Athlone Institute of Technology, Dublin Road, Bunnavally, Athlone and Co. Westmeath, Ireland.
| | - Noel M Gately
- Materials Research Institute, Athlone Institute of Technology, Dublin Road, Bunnavally, Athlone and Co. Westmeath, Ireland.
| | - Ian Major
- Materials Research Institute, Athlone Institute of Technology, Dublin Road, Bunnavally, Athlone and Co. Westmeath, Ireland.
| | - John G Lyons
- Faculty of Engineering and Informatics, Athlone Institute of Technology, Dublin Road, Bunnavally, Athlone, Co. Westmeath, Ireland.
| |
Collapse
|