Rizzarelli P, Leanza M, Rapisarda M. Investigations into the characterization, degradation, and applications of biodegradable polymers by mass spectrometry. MASS SPECTROMETRY REVIEWS 2023. [PMID: 38014928 DOI: 10.1002/mas.21869] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Grants] [Track Full Text] [Subscribe] [Scholar Register] [Received: 06/22/2023] [Revised: 10/10/2023] [Accepted: 11/08/2023] [Indexed: 11/29/2023]
Abstract
Biodegradable polymers have been getting more and more attention because of their contribution to the plastic pollution environmental issues and to move towards a circular economy. Nevertheless, biodegradable materials still exhibit various disadvantages restraining a widespread use in the market. Therefore, additional research efforts are required to improve their performance. Mass spectrometry (MS) affords a relevant contribution to optimize biodegradable polymer synthesis, to confirm macromolecular structures, to examine along the time the progress of degradation processes and highlight advantages and drawbacks in the extensive applications. This review aims to provide an overview of the MS investigations carried out to support the synthesis of biodegradable polymers, with helpful information on undesirable products or polymerization mechanism, to understand deterioration pathways by the structure of degradation products and to follow drug release and pharmacokinetic. Additionally, it summarizes MS studies addressed on environmental and health issues related to the extensive use of plastic materials, that is, potential migration of additives or microplastics identification and quantification. The paper is focused on the most significant studies relating to synthetic and microbial biodegradable polymers published in the last 15 years, not including agro-polymers such as proteins and polysaccharides.
Collapse
Affiliation(s)
- Paola Rizzarelli
- Consiglio Nazionale delle Ricerche (CNR), Istituto per i Polimeri Compositi e Biomateriali (IPCB), ede Secondaria di Catania, Catania, Italy
| | - Melania Leanza
- Consiglio Nazionale delle Ricerche (CNR), Istituto per i Polimeri Compositi e Biomateriali (IPCB), ede Secondaria di Catania, Catania, Italy
| | - Marco Rapisarda
- Consiglio Nazionale delle Ricerche (CNR), Istituto per i Polimeri Compositi e Biomateriali (IPCB), ede Secondaria di Catania, Catania, Italy
| |
Collapse
|
2
|
Mohammed-Sadhakathullah AHM, Paulo-Mirasol S, Torras J, Armelin E. Advances in Functionalization of Bioresorbable Nanomembranes and Nanoparticles for Their Use in Biomedicine. Int J Mol Sci 2023; 24:10312. [PMID: 37373461 PMCID: PMC10299464 DOI: 10.3390/ijms241210312] [Citation(s) in RCA: 1] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Grants] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 05/30/2023] [Revised: 06/15/2023] [Accepted: 06/16/2023] [Indexed: 06/29/2023] Open
Abstract
Bioresorbable nanomembranes (NMs) and nanoparticles (NPs) are powerful polymeric materials playing an important role in biomedicine, as they can effectively reduce infections and inflammatory clinical patient conditions due to their high biocompatibility, ability to physically interact with biomolecules, large surface area, and low toxicity. In this review, the most common bioabsorbable materials such as those belonging to natural polymers and proteins for the manufacture of NMs and NPs are reviewed. In addition to biocompatibility and bioresorption, current methodology on surface functionalization is also revisited and the most recent applications are highlighted. Considering the most recent use in the field of biosensors, tethered lipid bilayers, drug delivery, wound dressing, skin regeneration, targeted chemotherapy and imaging/diagnostics, functionalized NMs and NPs have become one of the main pillars of modern biomedical applications.
Collapse
Affiliation(s)
- Ahammed H. M. Mohammed-Sadhakathullah
- Departament d’Enginyeria Química, EEBE, Universitat Politècnica de Catalunya, C/Eduard Maristany, 10-14, Ed. I.2, 08019 Barcelona, Spain; (A.H.M.M.-S.); (S.P.-M.)
- Barcelona Research Center for Multiscale Science and Engineering, Universitat Politècnica de Catalunya, C/Eduard Maristany, 10-14, Ed. I.S, 08019 Barcelona, Spain
| | - Sofia Paulo-Mirasol
- Departament d’Enginyeria Química, EEBE, Universitat Politècnica de Catalunya, C/Eduard Maristany, 10-14, Ed. I.2, 08019 Barcelona, Spain; (A.H.M.M.-S.); (S.P.-M.)
- Barcelona Research Center for Multiscale Science and Engineering, Universitat Politècnica de Catalunya, C/Eduard Maristany, 10-14, Ed. I.S, 08019 Barcelona, Spain
| | - Juan Torras
- Departament d’Enginyeria Química, EEBE, Universitat Politècnica de Catalunya, C/Eduard Maristany, 10-14, Ed. I.2, 08019 Barcelona, Spain; (A.H.M.M.-S.); (S.P.-M.)
- Barcelona Research Center for Multiscale Science and Engineering, Universitat Politècnica de Catalunya, C/Eduard Maristany, 10-14, Ed. I.S, 08019 Barcelona, Spain
| | - Elaine Armelin
- Departament d’Enginyeria Química, EEBE, Universitat Politècnica de Catalunya, C/Eduard Maristany, 10-14, Ed. I.2, 08019 Barcelona, Spain; (A.H.M.M.-S.); (S.P.-M.)
- Barcelona Research Center for Multiscale Science and Engineering, Universitat Politècnica de Catalunya, C/Eduard Maristany, 10-14, Ed. I.S, 08019 Barcelona, Spain
| |
Collapse
|
3
|
Rizzarelli P, Rapisarda M. Matrix-Assisted Laser Desorption and Electrospray Ionization Tandem Mass Spectrometry of Microbial and Synthetic Biodegradable Polymers. Polymers (Basel) 2023; 15:polym15102356. [PMID: 37242931 DOI: 10.3390/polym15102356] [Citation(s) in RCA: 3] [Impact Index Per Article: 3.0] [Reference Citation Analysis] [Abstract] [Key Words] [Grants] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 04/04/2023] [Revised: 05/10/2023] [Accepted: 05/16/2023] [Indexed: 05/28/2023] Open
Abstract
The in-depth structural and compositional investigation of biodegradable polymeric materials, neat or partly degraded, is crucial for their successful applications. Obviously, an exhaustive structural analysis of all synthetic macromolecules is essential in polymer chemistry to confirm the accomplishment of a preparation procedure, identify degradation products originating from side reactions, and monitor chemical-physical properties. Advanced mass spectrometry (MS) techniques have been increasingly applied in biodegradable polymer studies with a relevant role in their further development, valuation, and extension of application fields. However, single-stage MS is not always sufficient to identify unambiguously the polymer structure. Thus, tandem mass spectrometry (MS/MS) has more recently been employed for detailed structure characterization and in degradation and drug release monitoring of polymeric samples, among which are biodegradable polymers. This review aims to run through the investigations carried out by the soft ionization technique matrix-assisted laser desorption/ionization mass spectrometry (MALDI-MS) and electrospray ionization mass spectrometry (ESI-MS) MS/MS in biodegradable polymers and present the resulting information.
Collapse
Affiliation(s)
- Paola Rizzarelli
- Institute for Polymers, Composites and Biomaterials, Consiglio Nazionale delle Ricerche (CNR), Via Paolo Gaifami 18, 95126 Catania, Italy
| | - Marco Rapisarda
- Institute for Polymers, Composites and Biomaterials, Consiglio Nazionale delle Ricerche (CNR), Via Paolo Gaifami 18, 95126 Catania, Italy
| |
Collapse
|
4
|
Tian R, Li K, Lin Y, Lu C, Duan X. Characterization Techniques of Polymer Aging: From Beginning to End. Chem Rev 2023; 123:3007-3088. [PMID: 36802560 DOI: 10.1021/acs.chemrev.2c00750] [Citation(s) in RCA: 4] [Impact Index Per Article: 4.0] [Reference Citation Analysis] [Abstract] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 02/22/2023]
Abstract
Polymers have been widely applied in various fields in the daily routines and the manufacturing. Despite the awareness of the aggressive and inevitable aging for the polymers, it still remains a challenge to choose an appropriate characterization strategy for evaluating the aging behaviors. The difficulties lie in the fact that the polymer features from the different aging stages require different characterization methods. In this review, we present an overview of the characterization strategies preferable for the initial, accelerated, and late stages during polymer aging. The optimum strategies have been discussed to characterize the generation of radicals, variation of functional groups, substantial chain scission, formation of low-molecular products, and deterioration in the polymers' macro-performances. In view of the advantages and the limitations of these characterization techniques, their utilization in a strategic approach is considered. In addition, we highlight the structure-property relationship for the aged polymers and provide available guidance for lifetime prediction. This review could allow the readers to be knowledgeable of the features for the polymers in the different aging stages and provide access to choose the optimum characterization techniques. We believe that this review will attract the communities dedicated to materials science and chemistry.
Collapse
Affiliation(s)
- Rui Tian
- State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology, Beijing 100029, China
| | - Kaitao Li
- State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology, Beijing 100029, China
| | - Yanjun Lin
- State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology, Beijing 100029, China
- School of Chemical Engineering, Qinghai University, Xining 810016, China
| | - Chao Lu
- State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology, Beijing 100029, China
- Green Catalysis Center, College of Chemistry, Zhengzhou University, Zhengzhou 450001, China
| | - Xue Duan
- State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology, Beijing 100029, China
| |
Collapse
|
5
|
Brzeska J, Jasik G, Sikorska W, Mendrek B, Karczewski J, Kowalczuk M, Rutkowska M. Susceptibility to Degradation in Soil of Branched Polyesterurethane Blends with Polylactide and Starch. Polymers (Basel) 2022; 14:polym14102086. [PMID: 35631968 PMCID: PMC9144702 DOI: 10.3390/polym14102086] [Citation(s) in RCA: 1] [Impact Index Per Article: 0.5] [Reference Citation Analysis] [Abstract] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 03/30/2022] [Revised: 05/14/2022] [Accepted: 05/17/2022] [Indexed: 02/04/2023] Open
Abstract
A very important method of reducing the amount of polymer waste in the environment is the introduction to the market of polymers susceptible to degradation under the influence of environmental factors. This paper presents the results of testing the susceptibility to degradation in soil of branched polyesterurethane (PUR) based on poly([R,S]-3-hydroxybutyrate) (R,S-PHB), modified with poly([D,L]-lactide) (PLA) and starch (St). Weight losses of samples and changes in surface morphology (SEM, OM and contact angle system) with simultaneously only slight changes in molecular weight (GPC), chemical structure (FTIR and 1HNMR) and thermal properties (DSC) indicate that these materials are subject to enzymatic degradation caused by the presence of microorganisms in the soil. Chemical modification of branched polyesterurethanes with R,S-PHB and their physical blending with small amounts of PLA and St resulted in a slow but progressive degradation of the samples.
Collapse
Affiliation(s)
- Joanna Brzeska
- Department of Industrial Product Quality and Chemistry, Gdynia Maritime University, 83 Morska Street, 81-225 Gdynia, Poland;
- Correspondence: (J.B.); (M.K.)
| | - Grzegorz Jasik
- Non-Food and Packaging Laboratory, J.S. Hamilton Poland Sp. z o.o., Chwaszczynska Street 180, 81-571 Gdynia, Poland;
| | - Wanda Sikorska
- Centre of Polymer and Carbon Materials, Polish Academy of Sciences, 34 M. Curie-Sklodowska Street, 41-819 Zabrze, Poland; (W.S.); (B.M.)
| | - Barbara Mendrek
- Centre of Polymer and Carbon Materials, Polish Academy of Sciences, 34 M. Curie-Sklodowska Street, 41-819 Zabrze, Poland; (W.S.); (B.M.)
| | - Jakub Karczewski
- Advanced Materials Center, Gdansk University of Technology, Narutowicza Street 11–12, 80-223 Gdansk, Poland;
- Faculty of Applied Physics and Mathematics, Institute of Nanotechnology and Materials Engineering, Gdansk University of Technology, Narutowicza Street 11-12, 80-223 Gdansk, Poland
| | - Marek Kowalczuk
- Centre of Polymer and Carbon Materials, Polish Academy of Sciences, 34 M. Curie-Sklodowska Street, 41-819 Zabrze, Poland; (W.S.); (B.M.)
- Correspondence: (J.B.); (M.K.)
| | - Maria Rutkowska
- Department of Industrial Product Quality and Chemistry, Gdynia Maritime University, 83 Morska Street, 81-225 Gdynia, Poland;
| |
Collapse
|
6
|
Rizzarelli P, La Carta S, Mirabella EF, Rapisarda M, Impallomeni G. Sequencing Biodegradable and Potentially Biobased Polyesteramide of Sebacic Acid and 3-Amino-1-propanol by MALDI TOF-TOF Tandem Mass Spectrometry. Polymers (Basel) 2022; 14:polym14081500. [PMID: 35458250 PMCID: PMC9032766 DOI: 10.3390/polym14081500] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 03/15/2022] [Revised: 04/04/2022] [Accepted: 04/05/2022] [Indexed: 12/10/2022] Open
Abstract
Biodegradable and potentially biobased polyesteramide oligomers (PEA-Pro), obtained from melt condensation of sebacic acid and 3-amino-1-propanol, were characterized by nuclear magnetic resonance (NMR), matrix assisted laser desorption/ionization-time of flight/time of flight-mass spectrometry/mass spectrometry (MALDI-TOF/TOF-MS/MS), thermogravimetric analysis (TGA), and pyrolysis-gas chromatography/mass spectrometry (Py-GC/MS). NMR analysis showed the presence of hydroxyl and amino terminal groups as well as carboxylic groups of the sebacate moiety. Hydroxyl and carboxyl termination had the same abundance, while the amine termination was 2.7-times less frequent. Information regarding the fragmentation pathways and ester/amide bond sequences was obtained by MALDI-TOF/TOF-MS/MS analysis performed on sodiated adducts of cyclic species and linear oligomers. Different end groups did not influence the observed fragmentation. Three fragmentation pathways were recognized. The β-hydrogen-transfer rearrangement, which leads to the selective scission of the –O–CH2– bonds, was the main mechanism. Abundant product ions originating from –CH2–CH2– (β–γ) bond cleavage in the sebacate moiety and less abundant ions formed by –O–CO– cleavages were also detected. TGA showed a major weight loss (74%) at 381 °C and a second degradation step (22% weight loss) at 447 °C. Py-GC/MS performed in the temperature range of 350–400 °C displayed partial similarity between the degradation products and the main fragments detected in the MALDI-TOF/TOF-MS/MS experiments. Degradation products derived from amide bonds were related to the formation of CN groups, in agreement with the literature.
Collapse
Affiliation(s)
- Paola Rizzarelli
- Istituto per i Polimeri, Compositi e Biomateriali, Consiglio Nazionale delle Ricerche, Via Paolo Gaifami 18, 95126 Catania, Italy; (E.F.M.); (M.R.); (G.I.)
- Correspondence:
| | - Stefania La Carta
- STMicroelectronics Srl, Stradale Primosole, 50, 95121 Catania, Italy;
| | - Emanuele Francesco Mirabella
- Istituto per i Polimeri, Compositi e Biomateriali, Consiglio Nazionale delle Ricerche, Via Paolo Gaifami 18, 95126 Catania, Italy; (E.F.M.); (M.R.); (G.I.)
| | - Marco Rapisarda
- Istituto per i Polimeri, Compositi e Biomateriali, Consiglio Nazionale delle Ricerche, Via Paolo Gaifami 18, 95126 Catania, Italy; (E.F.M.); (M.R.); (G.I.)
| | - Giuseppe Impallomeni
- Istituto per i Polimeri, Compositi e Biomateriali, Consiglio Nazionale delle Ricerche, Via Paolo Gaifami 18, 95126 Catania, Italy; (E.F.M.); (M.R.); (G.I.)
| |
Collapse
|
7
|
Fouquet TNJ, Amalian JA, Aniel N, Carvin-Sergent I, Issa S, Poyer S, Crozet D, Giusti P, Gigmes D, Trimaille T, Charles L. Reactive Desorption Electrospray Ionization Mass Spectrometry To Determine Intrinsic Degradability of Poly(lactic- co-glycolic acid) Chains. Anal Chem 2021; 93:12041-12048. [PMID: 34431672 DOI: 10.1021/acs.analchem.1c02280] [Citation(s) in RCA: 3] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/30/2022]
Abstract
Because of its speed, sensitivity, and ability to scrutinize individual species, mass spectrometry (MS) has become an essential tool in analytical strategies aimed at studying the degradation behavior of polyesters. MS analyses can be performed prior to the degradation event for structural characterization of initial substrates or after it has occurred to measure the decreasing size of products as a function of time. Here, we show that MS can also be usefully employed during the degradation process by online monitoring the chain solvolysis induced by reactive desorption electrospray ionization (DESI). Cleavage of ester bonds in random copolymers of lactic acid (LA) and glycolic acid (GA) was achieved by electrospraying methanol-containing NaOH onto the substrates. Experimental conditions were optimized to generate methanolysis products of high abundance so that mass spectra can be conveniently processed using Kendrick-based approaches. The same reactive-DESI performance was demonstrated for two sample preparations, solvent casting for soluble samples or pressed pellets for highly crystalline substrates, permitting to compare polymers with LA/GA ratios ranging from 100/0 to 5/95. Analysis of sample fractions collected by size exclusion chromatography showed that methanolysis occurs independently of the original chain size, so data recorded for poly(LA-co-GA) (PLAGA) copolymers with the average molecular weight ranging from 10 to 180 kDa could be safely compared. The average mass of methanolysis products was observed to decrease linearly (R2 = 0.9900) as the GA content increases in PLAGA substrates, consistent with the susceptibility of ester bonds toward solvolysis being higher in GA than in LA. Because DESI only explores the surface of solids, these data do not reflect bulk degradability of the copolymers but, instead, their relative degradability at the molecular level. Based on a "reactive-DESI degradability scale" such as that established here for PLAGA, the proposed method offers interesting perspectives to qualify intrinsic degradability of different polyesters and evaluate their erosion susceptibility or to determine the degradability of those polymers known to degrade via erosion only.
Collapse
Affiliation(s)
- Thierry N J Fouquet
- Research Institute for Sustainable Chemistry, National Institute of Advanced Industrial Science and Technology (AIST), Tsukuba, Ibaraki 305-8565, Japan
| | - Jean-Arthur Amalian
- Aix Marseille Université, CNRS, UMR7273, Institut de Chimie Radicalaire, Marseille 13397, France
| | - Nathan Aniel
- Aix Marseille Université, CNRS, UMR7273, Institut de Chimie Radicalaire, Marseille 13397, France
| | - Isaure Carvin-Sergent
- Aix Marseille Université, CNRS, UMR7273, Institut de Chimie Radicalaire, Marseille 13397, France
| | - Sébastien Issa
- Aix Marseille Université, CNRS, UMR7273, Institut de Chimie Radicalaire, Marseille 13397, France
| | - Salomé Poyer
- Aix Marseille Université, CNRS, UMR7273, Institut de Chimie Radicalaire, Marseille 13397, France
| | - Delphine Crozet
- Total Refining and Chemicals, Total Research & Technology Gonfreville, Harfleur 76700, France
| | - Pierre Giusti
- Total Refining and Chemicals, Total Research & Technology Gonfreville, Harfleur 76700, France.,International Joint laboratory-iC2MC: Complex Matrices Molecular Characterization, Harfleur 76700, France
| | - Didier Gigmes
- Aix Marseille Université, CNRS, UMR7273, Institut de Chimie Radicalaire, Marseille 13397, France
| | - Thomas Trimaille
- Aix Marseille Université, CNRS, UMR7273, Institut de Chimie Radicalaire, Marseille 13397, France
| | - Laurence Charles
- Aix Marseille Université, CNRS, UMR7273, Institut de Chimie Radicalaire, Marseille 13397, France
| |
Collapse
|
8
|
Fouquet TNJ, Pizzala H, Rollet M, Crozet D, Giusti P, Charles L. Mass Spectrometry-Based Analytical Strategy for Comprehensive Molecular Characterization of Biodegradable Poly(lactic- co-glycolic Acid) Copolymers. JOURNAL OF THE AMERICAN SOCIETY FOR MASS SPECTROMETRY 2020; 31:1554-1562. [PMID: 32510219 DOI: 10.1021/jasms.0c00137] [Citation(s) in RCA: 4] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Subscribe] [Scholar Register] [Indexed: 06/11/2023]
Abstract
An analytical methodology with mass spectrometry as the core technique was developed for precise characterization of end groups, size, and co-monomeric composition of poly(lactic-co-glycolic acid) (PLGA) copolymers, as a preliminary step to qualify their biodegradability. Four PLGA samples were studied, with GA molar content varying from 0 to 50% and Mw ranging from 18 to 75 kg mol-1 according to the supplier. Size exclusion chromatography (SEC) and liquid state nuclear magnetic resonance (NMR) were used as either complementary or validation techniques. As confirmed by tandem mass spectrometry (MS/MS) experiments, macrocycles were most prominent in the low mass range. Nevertheless, elemental compositions derived from high resolution (HR) mass measurements of linear species were consistent with chain terminations revealed by NMR. Off-line coupling of SEC with matrix-assisted laser desorption/ionization mass spectrometry (MALDI-MS) permitted calibration curves to be built based on absolute molecular weights and, although slightly overestimated, so-obtained Mn and Mw values compared well with SEC and NMR results. Homogeneity of the co-monomeric content of all chains within each PLGA sample was demonstrated using surface-assisted laser desorption/ionization in a reactive mode (reactive-SALDI), a newly developed technique that takes advantage of residual acid on desorption ionization using through-hole alumina membrane (DIUTHAME) chips to induce dissociation of high-molecular-weight polymers containing cleavable C-O bonds. All HRMS data were best handled with Kendrick analysis, which helped reveal minor species and allowed automated computation of congested mass spectra.
Collapse
Affiliation(s)
- Thierry N J Fouquet
- Research Institute for Sustainable Chemistry, National Institute of Advanced Industrial Science and Technology (AIST), Tsukuba, Tsukuba, Ibaraki 305-8565, Japan
| | - Hélène Pizzala
- Aix Marseille Université-CNRS, Institut de Chimie Radicalaire, 13397 Marseille, France
| | - Marion Rollet
- Aix Marseille Université-CNRS, Institut de Chimie Radicalaire, 13397 Marseille, France
| | - Delphine Crozet
- Total Refining and Chemicals, Total Research & Technology Gonfreville, 76700 Harfleur, France
| | - Pierre Giusti
- Total Refining and Chemicals, Total Research & Technology Gonfreville, 76700 Harfleur, France
- International Joint Laboratory - iC2MC: Complex Matrices Molecular Characterization, 76700 Harfleur, France
| | - Laurence Charles
- Aix Marseille Université-CNRS, Institut de Chimie Radicalaire, 13397 Marseille, France
| |
Collapse
|