Paolone G, Formiga S, De Palma F, Abbruzzese L, Chirico L, Scolavino S, Goracci C, Cantatore G, Vichi A. Color stability of resin-based composites: Staining procedures with liquids-A narrative review. J ESTHET RESTOR DENT 2022; 34:865-887. [PMID: 35396818 DOI: 10.1111/jerd.12912] [Citation(s) in RCA: 24] [Impact Index Per Article: 12.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 08/07/2021] [Revised: 01/30/2022] [Accepted: 03/24/2022] [Indexed: 12/12/2022]
Abstract
OBJECTIVE The objective of this study was to review the experimental staining procedures performed in in-vitro studies for evaluating color stability of resin-based composites used for direct restorations. OVERVIEW A review was performed with the purpose to identify in vitro procedures carried out to establish staining and color stability of resin-based composites used for direct restorations. A literature search was performed on four online databases (PubMed, Scopus, Embase and Web of Science) for articles published from January 1st 2001 till March 20th 2021, using a combination of free words and Medical Subject Headings (MESH) terms: "Composite Resins" AND "Color Stability" OR "Staining." Two reviewers screened titles and/or abstracts of 1728 unique studies. In total, 208 studies were selected for full-text reading, from which 178 were included in the review. The assessed variables were specimen dimensions, shape, and surface finishing; time before immersion; staining media type, dwell time, temperature and renewal interval; type of composite; color and translucency assessment parameters and measuring system. One hundred and seventy-eight articles analyzed color stability with staining liquids. Coffee was the most used staining medium (n = 102), followed by tea (n = 61), and red wine (n = 55). A disc-shaped specimen was used in most studies (n = 170) with a 2 mm thickness (n = 116). Spectrophotometers were the most used color assessment devices (n = 154), followed by colorimeters (n = 17). Color differences were quantified with ΔE (n = 154), ΔE00 (n = 23). Acceptability and or perceptibility thresholds were also taken into consideration (n = 126). CONCLUSIONS The large variety of staining procedure suggests the need for standardization. CLINICAL SIGNIFICANCE Aesthetic failure due to discoloration is a relevant clinical problem. Evaluating benefits and drawbacks of resin based composites artificial staining procedures will improve to predict materials clinical performances.
Collapse
Affiliation(s)
- Gaetano Paolone
- Dental School, IRCCS San Raffaele Hospital, Vita-Salute University, Milan, Italy
| | - Sara Formiga
- Dental School, IRCCS San Raffaele Hospital, Vita-Salute University, Milan, Italy
| | - Francesca De Palma
- Dental School, IRCCS San Raffaele Hospital, Vita-Salute University, Milan, Italy
| | - Luca Abbruzzese
- Dental School, IRCCS San Raffaele Hospital, Vita-Salute University, Milan, Italy
| | - Luca Chirico
- Dental School, IRCCS San Raffaele Hospital, Vita-Salute University, Milan, Italy
| | | | - Cecilia Goracci
- Department of Medical Biotechnologies, University of Siena, Siena, Italy
| | - Giuseppe Cantatore
- Dental School, IRCCS San Raffaele Hospital, Vita-Salute University, Milan, Italy
| | | |
Collapse
|
2
|
Impact of thermocycling on mechanical properties and discoloration of veneering composite resins after storage in various staining media. J Prosthet Dent 2021; 125:940-945. [DOI: 10.1016/j.prosdent.2020.03.030] [Citation(s) in RCA: 7] [Impact Index Per Article: 2.3] [Reference Citation Analysis] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 05/15/2019] [Revised: 03/23/2020] [Accepted: 03/23/2020] [Indexed: 11/23/2022]
|
3
|
Souza LS, Donato TR, Cerqueira GA, Cavalcanti AN, Mathias P. Color stability of an artificially aged nanofilled composite resin post-cured with different techniques. J Dent Res Dent Clin Dent Prospects 2021; 15:53-58. [PMID: 33927842 PMCID: PMC8058154 DOI: 10.34172/joddd.2021.010] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Journal Information] [Subscribe] [Scholar Register] [Received: 06/04/2020] [Accepted: 12/07/2020] [Indexed: 11/21/2022] Open
Abstract
Background. Post-cured composite resins exhibit improvements in physical and mechanical properties due to additional polymerization conversion. However, the post-curing techniques might influence the color stability of composite resin materials. Thus, this study evaluated the color stability of a nanofilled composite resin (Filtek Z350 XT - 3M ESPE) subjected to different post-curing techniques. Methods. Sixty samples (color A2) were randomly allocated to six experimental groups (n=10): G1: photoactivation (P) (control); G2: P + microwave oven with distilled water; G3: P + microwave oven without distilled water; G4: P + conventional oven; G5: P + dry-heat sterilizer; G6: P + steam autoclave. All the groups were stored in distilled water for 60 days and immersed daily in 5 mL of a coffee solution for 3 minutes. The color readings (CIEL*a*b* system) were performed at two different time intervals, initially and after 60 days, in a reflectance spectrophotometer (UV-2600; Shimadzu). The colorimetric readings were performed using the Color Analysis software (CIEL*a*b* system). Results. Group G6 exhibited significantly low values of total color change (ΔE=13.16). The control (ΔE=15.32) and G5 (ΔE=15.49) groups exhibited intermediate values, with no difference between them. In turn, the groups in which the resin was heated in a microwave (G2 ΔE=18.55 and G3 ΔE=19.45) exhibited the most significant color changes (one-way ANOVA and Tukey test, P ≤0.05). Conclusion. Steam autoclave post-polymerization increased the color stability of the nanofilled resin subjected to artificial aging and coffee immersion.
Collapse
Affiliation(s)
| | | | - Gabriela Alves Cerqueira
- Department of Restorative Dentistry , Faculty of Dentistry, Status University of Campinas, Brazil
| | | | - Paula Mathias
- Department of Clinical Dentistry, Faculty of Dentistry, Federal University of Bahia, Brazil
| |
Collapse
|
4
|
Surface Characteristics and Color Stability of Gingiva-Colored Resin Composites. MATERIALS 2020; 13:ma13112540. [PMID: 32503174 PMCID: PMC7321486 DOI: 10.3390/ma13112540] [Citation(s) in RCA: 5] [Impact Index Per Article: 1.3] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Subscribe] [Scholar Register] [Received: 04/20/2020] [Revised: 05/10/2020] [Accepted: 06/01/2020] [Indexed: 11/30/2022]
Abstract
The purpose of this study was to investigate the surface characteristics and color stability of gingiva-colored composite restorative materials (Anaxgum—ANG, Ceramage—CMG and Gradia Gum—GRG). The microstructure, composition, degree of conversion (DC %) and 3D roughness (Sa, Sz, Sdr, Sc) were examined by LV-SEM/EDS, ATR-FTIR and optical profilometry, respectively. For the color stability (CIE L*, a*, b* system) and hardness (HV), measurements were performed at baseline and after 30 days storage in distilled water, coffee and red wine. The ANG and GRG contain prepolymerized particles in aromatic and aliphatic resin matrices, respectively, whereas CMG contains inorganic zirconia silicate/silica particles, in an aromatic resin matrix, with a smaller particle size and a higher surface area fraction. Urethane monomers were mainly identified in CMG and GRG. The DC% showed statistically insignificant differences between the materials. The same applied for the roughness parameters, except for the greatest Sdr in CMG. ANG showed a color difference (ΔE) of > 3.3 after immersion in all media, CMG in coffee and wine and GRG only in coffee. Sc was the only roughness parameter demonstrating correlations with the ΔL*, Δb* and ΔE*. The HV values showed insignificant differences between the storage conditions per material. There are important differences in the color stability of the materials tested, which were mostly affected by the roughness parameters due to variations in their microstructure.
Collapse
|
5
|
Polychronakis N, Lagouvardos P, Polyzois G, Sykaras N, Zoidis P. Color changes of polyetheretherketone (PEEK) and polyoxymethelene (POM) denture resins on single and combined staining/cleansing action by CIELab and CIEDE2000 formulas. J Prosthodont Res 2019; 64:159-166. [PMID: 31852607 DOI: 10.1016/j.jpor.2019.06.005] [Citation(s) in RCA: 6] [Impact Index Per Article: 1.2] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 01/28/2019] [Revised: 05/27/2019] [Accepted: 06/17/2019] [Indexed: 10/25/2022]
Abstract
PURPOSE The purpose of study was to investigate the long-term effect of staining and/or cleansing solutions on the color stability of two non-metal removable partial denture materials. METHODS One hundred disks (25×3mm) of polyoxymethylene (POM) and polyetheretherketone (PEEK) were immersed in water, wine, coffee, cleanser and combo bath, simulating normal daily use. Color parameters in the CIELAB system was measured every 30 cycles up to 240 using a contact colorimeter and color differences estimated using ΔEab and ΔE00 formulas. Two-way repeated measures ANOVAs and regression analyses were performed at α=0.05. RESULTS Regression analysis indicated a strong R2 between color changes and number of cycles, for both materials. Tests of within-subjects effects for the ΔEab revealed significant differences among cycles and between the materials in the wine and coffee baths (p<0.001). Significant materialXcycles interactions were also recorded with all staining baths. ΔE00 values were lower than ΔEab up to 63.6%. Tests within and between-subjects effects for the ΔE00 gave similar but not the same with ΔEab results. CONCLUSIONS ΔE00 found to correlate well with ΔEab. Long term exposure of both materials showed a progressive discoloration in all except control baths. POM discolored more than PEEK in coffee, and combo baths but not in cleanser. Discoloration was smaller in combo bath (where a cleanser was also used) indicating the effectiveness of a cleanser to prevent long term discoloration of both materials.
Collapse
Affiliation(s)
- Nick Polychronakis
- Department of Prosthodontics, School of Dentistry, National and Kapodistrian University of Athens, Athens, Greece.
| | - Panagiotis Lagouvardos
- Department of Operative Dentistry, School of Dentistry, National and Kapodistrian University of Athens, Athens, Greece
| | - Gregory Polyzois
- Department of Prosthodontics, School of Dentistry, National and Kapodistrian University of Athens, Athens, Greece
| | - Nikitas Sykaras
- Department of Prosthodontics, School of Dentistry, National and Kapodistrian University of Athens, Athens, Greece
| | - Panagiotis Zoidis
- Department of Restorative Dental Sciences, Division of Prosthodontics, University of Florida College of Dentistry, Gainesville, FL, United States
| |
Collapse
|
6
|
Schürmann MG, Olms C. Shade Stability of Polymer-Infiltrated and Resin Nano Ceramics. Open Dent J 2018; 12:791-800. [PMID: 30450137 PMCID: PMC6198420 DOI: 10.2174/1745017901814010791] [Citation(s) in RCA: 4] [Impact Index Per Article: 0.7] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 03/18/2018] [Revised: 07/31/2018] [Accepted: 09/19/2018] [Indexed: 01/14/2023] Open
Abstract
BACKGROUND The esthetics plays an increasingly significant role in today's dentistry. OBJECTIVE The objective was to investigate the shade stability of a polymer-infiltrated and a resin nano ceramic in comparison to a conventional feldspar ceramic and an acrylate polymer. METHODS 20 specimens of each of the materials, CAD-Temp (CT), Mark II (M), VITA Enamic (VE) and Lava Ultimate (LU), were prepared using the standard method. These were divided into groups (n=5) and placed in the following stain solutions: Distilled water, coffee, Coca-Cola and red wine for 14 days. The shade of each specimen was measured before and after using a spectrophotometer (n=5). The data were analyzed using ANOVA and Tukey's test (p ≤ 0.05). RESULTS The largest ΔE mean values were observed in CT by Coca-Cola (4.38 ± 0.41), in M by coffee (5.95 ± 0.62), in VE (6.02 ± 0.78) and LU (8.61 ± 0.30) by red wine. LU had the largest and strongest overall shade differences (total score: SSC=16.95) and CT the least (SSC=8.74). Overall shade differences of VE (SSC=12.03) and M (SSC=12.48) were statistically indistinguishable. After 14 days, only Coca-Cola caused clinically relevant shade differences in CT (ΔE > 2.7); this was also caused by coffee, Coca-Cola and red wine in M and coffee and red wine in VE and LU. CONCLUSION On average, VE showed fewer shade differences than LU. After 14 days of immersion, shade differences which exceeded the clinical acceptance threshold of ΔE=2.7 were shown by CT in Coca-Cola, by M in coffee, Coca-Cola and red wine, and by VE and LU in coffee and red wine.
Collapse
Affiliation(s)
- Martin Gabriel Schürmann
- Department of Prosthodontics and Material Science, University of Leipzig, Liebigstr.12, 04103 Leipzig, Germany
| | - Constanze Olms
- Department of Prosthodontics and Material Science, University of Leipzig, Liebigstr.12, 04103 Leipzig, Germany
| |
Collapse
|
7
|
Zoidis P, Polychronakis N, Lagouvardos P, Polyzois G, Ngo HC. Evaluation of a Realistic Cleansing Protocol for Preventing Discoloration of Denture Resins. J Prosthodont 2018; 28:e89-e95. [PMID: 29468768 DOI: 10.1111/jopr.12763] [Citation(s) in RCA: 7] [Impact Index Per Article: 1.2] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Accepted: 11/16/2017] [Indexed: 11/28/2022] Open
Abstract
PURPOSE To evaluate the efficacy of a realistic staining/cleansing protocol for long-term prevention of discoloration of denture base resins. MATERIALS AND METHODS Sixty discs (20 × 2.5 mm) of auto- and heat-polymerizing denture acrylic resins were fabricated following manufacturer's instructions, polished on one side and stored in water (37°C) for 24 hours before they were assigned randomly into 6 groups (3 for each material, n = 10) to receive 220 cycles of three immersion protocols. Group A was immersed in the following baths: (1) filtered coffee at 45°C for 2 minutes, (2) tap water at 24°C for 20 seconds, (3) as bath 1, (4) as bath 2, (5) Corega Extradent cleansing solution at 45°C for 3 minutes, and (6) water at 24°C for 20 seconds. Group B was immersed in the four first baths of group A (without cleansing action) and group C in bath 1 for the cumulative action of 20 cycles (80 minutes in 45°C coffee) and bath 2 for 40 seconds. A noncontact optical interferometric profilometer was used for qualitative evaluation of the specimens and a contact colorimeter to estimate color change values (ΔΕ*ab) at baseline and every 20 cycles in the baths for a total of 220 cycles. Data were statistically analyzed using a 2-way-repeated measures ANOVA with Bonferoni multiple comparisons and trend analysis at α = 0.05 level of significance. RESULTS Data indicated changes in color from 1.7 to 14.2 ΔΕ*ab units. The highest values were related to the number of cycles and group B immersion protocol. Significant differences were found among immersion protocols (p < 0.001) and immersion cycles (p < 0.001) with a significant interaction between protocols and cycles (p < 0.001) but not between denture resins (p = 0.991). CONCLUSION The evaluated protocol A was found effective in preventing color changes in both denture resins even after a long period of action. Protocol C had a much lower staining effect on both resins than protocol B and behaved similarly to protocol A until 140 to 160 cycles. Therefore, it is probably not appropriate for use in short-term color stability experiments.
Collapse
Affiliation(s)
- Panagiotis Zoidis
- Department of Prosthodontics, Dental School, National and Kapodistrian University of Athens, Athens, Greece
| | - Nikolaos Polychronakis
- Department of Prosthodontics, Dental School, National and Kapodistrian University of Athens, Athens, Greece
| | - Panagiotis Lagouvardos
- Department of Operative Dentistry, Dental School, National and Kapodistrian University of Athens, Athens, Greece
| | - Gregory Polyzois
- Department of Prosthodontics, Dental School, National and Kapodistrian University of Athens, Athens, Greece
| | - Hien Chi Ngo
- Department of Preventive and Restorative Dentistry, College of Dental Medicine, University of Sharjha, Sharjha, United Arab Emirates
| |
Collapse
|
8
|
Xing W, Jiang T, Liang S, Sa Y, Wang Z, Chen X, Wang Y. Effect of in-office bleaching agents on the color changes of stained ceromers and direct composite resins. Acta Odontol Scand 2014; 72:1032-8. [PMID: 25196263 DOI: 10.3109/00016357.2014.946962] [Citation(s) in RCA: 9] [Impact Index Per Article: 0.9] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/13/2022]
Abstract
PURPOSE To evaluate the effect of two in-office bleaching agents on the color changes of two ceromers (Ceramage and Adoro SR) and one direct composite resin (Gradia Direct Anterior) after staining by tea and coffee. MATERIALS AND METHODS Twenty-four disk-shaped specimens were fabricated for each resin material and randomly divided into three groups (n = 8). The specimens were immersed in tea, coffee or deionized water, respectively, for 7 days. Each group was then equally divided into two sub-groups (n = 4), which were subjected to two in-office bleaching agents (BEYOND and Opalescence Boost), respectively. The color of the specimens was measured by a spectrophotometer at baseline, after staining and after bleaching. The color differences (ΔE values) between baseline and after treatments were calculated. RESULTS Statistical analysis indicated that the staining solution had significant influence on the color change of resin composites tested (p < 0.001). The discolorations of resin composites were perceptible after immersing in tea or coffee solutions (ΔE>2.0). There was no statistically significant difference between BEYOND and Opalescence Boost in stains removal from discolored resins (p = 0.550). The color changes in ΔE value between baseline and after bleaching were less than 2.0 for all resin composite groups. CONCLUSIONS Tea solution produces severe discoloration of three resin composites tested. The two in-office bleaching agents can effectively remove the stains from two ceromers and one direct composite resin tested in this study.
Collapse
Affiliation(s)
- Wenzhong Xing
- The State Key Laboratory Breeding Base of Basic Science of Stomatology (Hubei-MOST) & Key Laboratory of Oral Biomedicine Ministry of Education, School & Hospital of Stomatology, Wuhan University , Wuhan , PR China
| | | | | | | | | | | | | |
Collapse
|