1
|
Fendi F, Abdullah B, Suryani S, Usman AN, Tahir D. Development and application of hydroxyapatite-based scaffolds for bone tissue regeneration: A systematic literature review. Bone 2024; 183:117075. [PMID: 38508371 DOI: 10.1016/j.bone.2024.117075] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Journal Information] [Submit a Manuscript] [Subscribe] [Scholar Register] [Received: 01/12/2024] [Revised: 03/14/2024] [Accepted: 03/15/2024] [Indexed: 03/22/2024]
Abstract
Hydroxyapatite [HA, Ca10(PO4)6(OH)2], with its robust biocompatibility and bioactivity, has found extensive utility in bone grafting, replacement therapies, and supplemental medical materials. HA is highly regarded for its osteoconductive properties because it boasts hydrophilicity, nontoxicity, non-allergenicity, and non-mutagenicity. Nevertheless, HA's intrinsic mechanical weakness has spurred efforts to enhance its properties. This enhancement is achieved through ion incorporation, with elements such as magnesium, zinc, lithium, strontium, boron, and others being integrated into the HA structure. In the domain of orthopedics, HA-based scaffolds have emerged as a solution for addressing prevalent issues like bone deformities and defects stemming from congenital anomalies, injuries, trauma, infections, or tumors. The fabrication of three-dimensional scaffolds (3D scaffolds) has enabled advancements in bone regeneration and replacement, with a focus on practical applications such as repairing calvarial, skull, and femoral defects. In vitro and in vivo assessments have substantiated the effectiveness of 3D scaffolds for bone defect repair, regeneration, and tissue engineering. Beyond bone-related applications, scaffolds demonstrate versatility in enhancing cartilage healing and serving as bioimplants. The wide array of scaffold applications underscores their ongoing potential for further development in the realm of medical science.
Collapse
Affiliation(s)
- Fendi Fendi
- Department of Physics, Hasanuddin University, Makassar 90245, Indonesia
| | - Bualkar Abdullah
- Department of Physics, Hasanuddin University, Makassar 90245, Indonesia
| | - Sri Suryani
- Department of Physics, Hasanuddin University, Makassar 90245, Indonesia
| | | | - Dahlang Tahir
- Department of Physics, Hasanuddin University, Makassar 90245, Indonesia.
| |
Collapse
|
2
|
Huo M, He S, Zhang Y, Liu Q, Liu M, Zhou G, Zhou P, Lu J. Mechano-driven intervertebral bone bridging via oriented mechanical stimulus in a twist metamaterial cage: An in silico study. Comput Biol Med 2024; 171:108149. [PMID: 38401455 DOI: 10.1016/j.compbiomed.2024.108149] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 07/17/2023] [Revised: 01/11/2024] [Accepted: 02/12/2024] [Indexed: 02/26/2024]
Abstract
Stiffer cages provide sufficient mechanical support but fail to promote bone ingrowth due to stress shielding. It remains challenging for fusion cage to satisfy both bone bridging and mechanical stability. Here we designed a fusion cage based on twist metamaterial for improved bone ingrowth, and proved its superiority to the conventional diagonal-based cage in silico. The fusion process was numerically reproduced via an injury-induced osteogenesis model and the mechano-driven bone remodeling algorithm, and the outcomes fusion effects were evaluated by the morphological features of the newly-formed bone and the biomechanical behaviors of the bone-cage composite. The twist-based cages exhibited oriented bone formation in the depth direction, in comparison to the diagonal-based cages. The axial stiffness of the bone-cage composites with twist-based cages was notably higher than that with diagonal-based cages; meanwhile, the ranges of motion of the twist-based fusion segment were lower. It was concluded that the twist metamaterial cages led to oriented bone ingrowth, superior mechanical stability of the bone-cage composite, and less detrimental impacts on the adjacent bones. More generally, metamaterials with a tunable displacement mode of struts might provide more design freedom in implant designs to offer customized mechanical stimulus for osseointegration.
Collapse
Affiliation(s)
- Mengke Huo
- State Key Laboratory of Digital Medical Engineering, School of Biological Science & Medical Engineering, Southeast University, Nanjing, China; Department of Mechanical Engineering, City University of Hong Kong, Hong Kong, China; CityU-Shenzhen Futian Research Institute, Shenzhen, China
| | - Siyuan He
- State Key Laboratory of Digital Medical Engineering, School of Biological Science & Medical Engineering, Southeast University, Nanjing, China.
| | - Yun Zhang
- State Key Laboratory of Digital Medical Engineering, School of Biological Science & Medical Engineering, Southeast University, Nanjing, China; Biomechanics Section, Department of Mechanical Engineering, KU Leuven, Leuven, Belgium
| | - Qing Liu
- State Key Laboratory of Digital Medical Engineering, School of Biological Science & Medical Engineering, Southeast University, Nanjing, China
| | - Mengxing Liu
- Shenzhen Mindray Bio-Medical Electronics Co., Ltd, Shenzhen, China; Wuhan Mindray Scientific Co., Ltd, Wuhan, China
| | - Guangquan Zhou
- State Key Laboratory of Digital Medical Engineering, School of Biological Science & Medical Engineering, Southeast University, Nanjing, China
| | - Ping Zhou
- State Key Laboratory of Digital Medical Engineering, School of Biological Science & Medical Engineering, Southeast University, Nanjing, China
| | - Jian Lu
- Department of Mechanical Engineering, City University of Hong Kong, Hong Kong, China; CityU-Shenzhen Futian Research Institute, Shenzhen, China; Centre for Advanced Structural Materials, City University of Hong Kong Shenzhen Research Institute, Greater Bay Joint Division, Shenyang National Laboratory for Materials Science, Shenzhen, China
| |
Collapse
|
3
|
Urzì O, Gasparro R, Costanzo E, De Luca A, Giavaresi G, Fontana S, Alessandro R. Three-Dimensional Cell Cultures: The Bridge between In Vitro and In Vivo Models. Int J Mol Sci 2023; 24:12046. [PMID: 37569426 PMCID: PMC10419178 DOI: 10.3390/ijms241512046] [Citation(s) in RCA: 24] [Impact Index Per Article: 12.0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 06/20/2023] [Revised: 07/19/2023] [Accepted: 07/21/2023] [Indexed: 08/13/2023] Open
Abstract
Although historically, the traditional bidimensional in vitro cell system has been widely used in research, providing much fundamental information regarding cellular functions and signaling pathways as well as nuclear activities, the simplicity of this system does not fully reflect the heterogeneity and complexity of the in vivo systems. From this arises the need to use animals for experimental research and in vivo testing. Nevertheless, animal use in experimentation presents various aspects of complexity, such as ethical issues, which led Russell and Burch in 1959 to formulate the 3R (Replacement, Reduction, and Refinement) principle, underlying the urgent need to introduce non-animal-based methods in research. Considering this, three-dimensional (3D) models emerged in the scientific community as a bridge between in vitro and in vivo models, allowing for the achievement of cell differentiation and complexity while avoiding the use of animals in experimental research. The purpose of this review is to provide a general overview of the most common methods to establish 3D cell culture and to discuss their promising applications. Three-dimensional cell cultures have been employed as models to study both organ physiology and diseases; moreover, they represent a valuable tool for studying many aspects of cancer. Finally, the possibility of using 3D models for drug screening and regenerative medicine paves the way for the development of new therapeutic opportunities for many diseases.
Collapse
Affiliation(s)
- Ornella Urzì
- Department of Biomedicine, Neuroscience and Advanced Diagnostics (Bi.N.D), Section of Biology and Genetics, University of Palermo, 90133 Palermo, Italy; (O.U.); (R.G.); (E.C.); (R.A.)
| | - Roberta Gasparro
- Department of Biomedicine, Neuroscience and Advanced Diagnostics (Bi.N.D), Section of Biology and Genetics, University of Palermo, 90133 Palermo, Italy; (O.U.); (R.G.); (E.C.); (R.A.)
| | - Elisa Costanzo
- Department of Biomedicine, Neuroscience and Advanced Diagnostics (Bi.N.D), Section of Biology and Genetics, University of Palermo, 90133 Palermo, Italy; (O.U.); (R.G.); (E.C.); (R.A.)
| | - Angela De Luca
- IRCCS Istituto Ortopedico Rizzoli, SC Scienze e Tecnologie Chirurgiche, 40136 Bologna, Italy; (A.D.L.); (G.G.)
| | - Gianluca Giavaresi
- IRCCS Istituto Ortopedico Rizzoli, SC Scienze e Tecnologie Chirurgiche, 40136 Bologna, Italy; (A.D.L.); (G.G.)
| | - Simona Fontana
- Department of Biomedicine, Neuroscience and Advanced Diagnostics (Bi.N.D), Section of Biology and Genetics, University of Palermo, 90133 Palermo, Italy; (O.U.); (R.G.); (E.C.); (R.A.)
| | - Riccardo Alessandro
- Department of Biomedicine, Neuroscience and Advanced Diagnostics (Bi.N.D), Section of Biology and Genetics, University of Palermo, 90133 Palermo, Italy; (O.U.); (R.G.); (E.C.); (R.A.)
| |
Collapse
|
4
|
Calazans Neto JV, Reis ACD, Valente MLDC. Osseointegration in additive-manufactured titanium implants: A systematic review of animal studies on the need for surface treatment. Heliyon 2023; 9:e17105. [PMID: 37484223 PMCID: PMC10361303 DOI: 10.1016/j.heliyon.2023.e17105] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Track Full Text] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Received: 09/19/2022] [Revised: 05/22/2023] [Accepted: 06/07/2023] [Indexed: 07/25/2023] Open
Abstract
The objective of the systematic review is to find an answer to a question: "Do surface treatments on titanium implants produced by additive manufacturing improve osseointegration, compared to untreated surfaces?". This review followed the Preferred Reporting Items for Systematic Review and Meta-Analysis (PRISMA 2020) and was registered in the International Prospective Register of Systematic Reviews (PROSPERO) (CRD42022321351). Searches were performed in PubMed, Scopus, Science Direct, Embase, and Google Scholar databases on March 22nd, 2022. Articles were chosen in 2 steps by 2 blinded reviewers based on previously selected inclusion criteria: articles in animals that addressed the influence of surface treatments on osseointegration in implants produced by additive manufacturing. Articles were excluded that (1) did not use titanium surface, 2) that did not evaluate surface treatments, 3) that did not described osseointegration, 4) Studies with only in vitro analyses, clinical studies, systematic reviews, book chapters, short communications, conference abstracts, case reports and personal opinions.). 1003 articles were found and, after applying the eligibility criteria, 17 were used for the construction of this review. All included studies found positive osseointegration results from performing surface treatments on titanium. The risk of bias was analyzed using the SYRCLE assessment tool. Surface treatments are proposed to promote changes in the microstructure and composition of the implant surface to favor the adhesion of bone cells responsible for osseointegration. It is observed that despite the benefits generated by the additive manufacturing process in the microstructure of the implant surface, surface treatments are still indispensable, as they can promote more suitable characteristics for bone-implant integration. It can be concluded that the surface treatments evaluated in this systematic review, performed on implants produced by additive manufacturing, optimize osseointegration, as it allows the creation of a micro-nano-textured structure that makes the surface more hydrophilic and allows better contact bone-implant.
Collapse
Affiliation(s)
| | | | - Mariana Lima da Costa Valente
- Corresponding author. Department of Dental Materials and Prosthodontics, Ribeirão Preto Dental School, FORP-USP. Av. Do Café, s/n, 14040Ribeirão Preto, Brazil.
| |
Collapse
|
5
|
Popkov A, Kononovich N, Dubinenko G, Gorbach E, Shastov A, Tverdokhlebov S, Popkov D. Long Bone Defect Filling with Bioactive Degradable 3D-Implant: Experimental Study. Biomimetics (Basel) 2023; 8:biomimetics8020138. [PMID: 37092390 PMCID: PMC10123725 DOI: 10.3390/biomimetics8020138] [Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [Abstract] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 02/27/2023] [Revised: 03/26/2023] [Accepted: 03/26/2023] [Indexed: 03/30/2023] Open
Abstract
Previously, 3D-printed bone grafts made of titanium alloy with bioactive coating has shown great potential for the restoration of bone defects. Implanted into a medullary canal titanium graft with cellular structure demonstrated stimulation of the reparative osteogenesis and successful osseointegration of the graft into a single bone-implant block. The purpose of this study was to investigate osseointegration of a 3D-printed degradable polymeric implant with cellular structure as preclinical testing of a new technique for bone defect restoration. During an experimental study in sheep, a 20 mm-long segmental tibial defect was filled with an original cylindrical implant with cellular structure made of polycaprolactone coated with hydroxyapatite. X-ray radiographs demonstrated reparative bone regeneration from the periosteum lying on the periphery of cylindrical implant to its center in a week after the surgery. Cellular structure of the implant was fully filled with newly-formed bone tissue on the 4th week after the surgery. The bone tissue regeneration from the proximal and distal bone fragments was evident on 3rd week. This provides insight into the use of bioactive degradable implants for the restoration of segmental bone defects. Degradable implant with bioactive coating implanted into a long bone segmental defect provides stimulation of reparative osteogenesis and osseointegration into the single implant-bone block.
Collapse
|
6
|
Wei J, Yan Y, Gao J, Li Y, Wang R, Wang J, Zou Q, Zuo Y, Zhu M, Li J. 3D-printed hydroxyapatite microspheres reinforced PLGA scaffolds for bone regeneration. MATERIALS SCIENCE & ENGINEERING. C, MATERIALS FOR BIOLOGICAL APPLICATIONS 2021; 133:112618. [PMID: 35031175 DOI: 10.1016/j.msec.2021.112618] [Citation(s) in RCA: 28] [Impact Index Per Article: 7.0] [Reference Citation Analysis] [Abstract] [Key Words] [MESH Headings] [Track Full Text] [Subscribe] [Scholar Register] [Received: 08/10/2021] [Revised: 10/13/2021] [Accepted: 12/14/2021] [Indexed: 01/01/2023]
Abstract
Bone tissue engineering scaffolds with similar composition, structure, and mechanical properties to natural bone are conducive to bone regeneration. The objective of this study was to prepare hydroxyapatite/poly (lactic-co-glycolic acid) (HA/PLGA) three-dimensional porous scaffolds with HA content close to natural bone and strong mechanical strength to promote osteogenesis. To achieve this, we modified HA microspheres with polyvinyl alcohol to create an inorganic filler to endow the HA/PLGA printing ink with higher HA content and excellent printing fluidity for 3D printing. We successfully printed a series of HA/PLGA scaffolds with different HA contents. The highest HA content reached 60 wt%, which is close to the mineral percentage in natural bone. The composition, structure, mechanical properties, and in vitro degradability of the fabricated scaffolds were systematically characterized. The cytocompatibility and osteogenic activity of the fabricated HA/PLGA scaffolds were evaluated by in vitro cell culture and rabbit femoral defect repair experiments in vivo. The results indicated that the HA/PLGA composite scaffold with 45 wt% HA had the highest compressive strength of more than 40 MPa, which was six times higher than that of the pure PLGA scaffold. The incorporation of HA microspheres into the PLGA matrix significantly improved the cell adhesion, proliferation, and osteogenic differentiation of bone marrow stem cells (BMSCs) cultured on the surface of the scaffolds. Animal experiments showed that the HA/PLGA composite with 45 wt% HA exhibited the best structure maintenance and osteogenic performance in vivo. The prepared HA/PLGA composite 3D scaffold with HA microsphere reinforcement has considerable application potential in the field of large bone defect repair.
Collapse
Affiliation(s)
- Jiawei Wei
- Research Center for Nano-Biomaterials, Analytical and Testing Center, Sichuan University, Chengdu 610064, PR China
| | - Yan Yan
- Research Center for Nano-Biomaterials, Analytical and Testing Center, Sichuan University, Chengdu 610064, PR China
| | - Jing Gao
- Research Center for Nano-Biomaterials, Analytical and Testing Center, Sichuan University, Chengdu 610064, PR China
| | - Yubao Li
- Research Center for Nano-Biomaterials, Analytical and Testing Center, Sichuan University, Chengdu 610064, PR China
| | - Ruili Wang
- State Key Laboratory for Modification of Chemical Fibers and Polymer Materials, College of Materials Science and Engineering, Donghua University, Shanghai 201620, PR China
| | - Jiexin Wang
- State Key Laboratory of Organic-Inorganic Composites, Beijing University of Chemical Technology, Beijing 100029, PR China
| | - Qin Zou
- Research Center for Nano-Biomaterials, Analytical and Testing Center, Sichuan University, Chengdu 610064, PR China
| | - Yi Zuo
- Research Center for Nano-Biomaterials, Analytical and Testing Center, Sichuan University, Chengdu 610064, PR China
| | - Meifang Zhu
- State Key Laboratory for Modification of Chemical Fibers and Polymer Materials, College of Materials Science and Engineering, Donghua University, Shanghai 201620, PR China.
| | - Jidong Li
- Research Center for Nano-Biomaterials, Analytical and Testing Center, Sichuan University, Chengdu 610064, PR China.
| |
Collapse
|
7
|
Baltatu MS, Sandu AV, Nabialek M, Vizureanu P, Ciobanu G. Biomimetic Deposition of Hydroxyapatite Layer on Titanium Alloys. MICROMACHINES 2021; 12:1447. [PMID: 34945297 PMCID: PMC8704239 DOI: 10.3390/mi12121447] [Citation(s) in RCA: 4] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Key Words] [Grants] [Track Full Text] [Download PDF] [Figures] [Subscribe] [Scholar Register] [Received: 11/04/2021] [Revised: 11/23/2021] [Accepted: 11/24/2021] [Indexed: 11/21/2022]
Abstract
Over the last decade, researchers have been concerned with improving metallic biomaterials with proper and suitable properties for the human body. Ti-based alloys are widely used in the medical field for their good mechanical properties, corrosion resistance and biocompatibility. The TiMoZrTa system (TMZT) evidenced adequate mechanical properties, was closer to the human bone, and had a good biocompatibility. In order to highlight the osseointegration of the implants, a layer of hydroxyapatite (HA) was deposited using a biomimetic method, which simulates the natural growth of the bone. The coatings were examined by scanning electron microscopy (SEM), X-ray diffraction (XRD), micro indentation tests and contact angle. The data obtained show that the layer deposited on TiMoZrTa (TMZT) support is hydroxyapatite. Modifying the surface of titanium alloys represents a viable solution for increasing the osseointegration of materials used as implants. The studied coatings demonstrate a positive potential for use as dental and orthopedic implants.
Collapse
Affiliation(s)
- Madalina Simona Baltatu
- Faculty of Materials Science and Engineering, Gheorghe Asachi Technical University of Iasi, 41 D. Mangeron Street, 700050 Iasi, Romania; (M.S.B.); (A.V.S.)
| | - Andrei Victor Sandu
- Faculty of Materials Science and Engineering, Gheorghe Asachi Technical University of Iasi, 41 D. Mangeron Street, 700050 Iasi, Romania; (M.S.B.); (A.V.S.)
- Romanian Inventors Forum, 3 Sf. P. Movila St, 700089 Iasi, Romania
| | - Marcin Nabialek
- Department of Physics, Częstochowa University of Technology, 42-200 Częstochowa, Poland;
| | - Petrica Vizureanu
- Faculty of Materials Science and Engineering, Gheorghe Asachi Technical University of Iasi, 41 D. Mangeron Street, 700050 Iasi, Romania; (M.S.B.); (A.V.S.)
| | - Gabriela Ciobanu
- Faculty of Chemical Engineering and Environmental Protection Cristofor Simionescu, Gheorghe Asachi Technical University of Iasi, 73 D. Mangeron Street, 700050 Iasi, Romania;
| |
Collapse
|
8
|
Oltean-Dan D, Dogaru GB, Jianu EM, Riga S, Tomoaia-Cotisel M, Mocanu A, Barbu-Tudoran L, Tomoaia G. Biomimetic Composite Coatings for Activation of Titanium Implant Surfaces: Methodological Approach and In Vivo Enhanced Osseointegration. MICROMACHINES 2021; 12:mi12111352. [PMID: 34832764 PMCID: PMC8618198 DOI: 10.3390/mi12111352] [Citation(s) in RCA: 4] [Impact Index Per Article: 1.0] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Download PDF] [Figures] [Subscribe] [Scholar Register] [Received: 10/02/2021] [Revised: 10/24/2021] [Accepted: 10/25/2021] [Indexed: 12/14/2022]
Abstract
Innovative nanomaterials are required for the coatings of titanium (Ti) implants to ensure the activation of Ti surfaces for improved osseointegration, enhanced bone fracture healing and bone regeneration. This paper presents a systematic investigation of biomimetic composite (BC) coatings on Ti implant surfaces in a rat model of a diaphyseal femoral fracture. Methodological approaches of surface modification of the Ti implants via the usual joining methods (e.g., grit blasting and acid etching) and advanced physicochemical coating via a self-assembled dip-coating method were used. The biomimetic procedure used multi-substituted hydroxyapatite (ms-HAP) HAP-1.5 wt% Mg-0.2 wt% Zn-0.2 wt% Si nanoparticles (NPs), which were functionalized using collagen type 1 molecules (COL), resulting in ms-HAP/COL (core/shell) NPs that were embedded into a polylactic acid (PLA) matrix and finally covered with COL layers, obtaining the ms-HAP/COL@PLA/COL composite. To assess the osseointegration issue, first, the thickness, surface morphology and roughness of the BC coating on the Ti implants were determined using AFM and SEM. The BC-coated Ti implants and uncoated Ti implants were then used in Wistar albino rats with a diaphyseal femoral fracture, both in the absence and the presence of high-frequency pulsed electromagnetic shortwave (HF-PESW) stimulation. This study was performed using a bone marker serum concentration and histological and computer tomography (micro-CT) analysis at 2 and 8 weeks after surgical implantation. The implant osseointegration was evaluated through the bone–implant contact (BIC). The bone–implant interface was investigated using FE-SEM images and EDX spectra of the retrieved surgical implants at 8 weeks in the four animal groups. The obtained results showed significantly higher bone–implants contact and bone volume per tissue volume, as well as a greater amount of newly formed bone, in the BC-coated Ti implants than in the uncoated Ti implants. Direct bone–implant contact was also confirmed via histological examination. The results of this study confirmed that these biomimetic composite coatings on Ti implants were essential for a significant enhancement of osseointegration of BC-coated Ti implants and bone regeneration. This research provides a novel strategy for the treatment of bone fractures with possible orthopedic applications.
Collapse
Affiliation(s)
- Daniel Oltean-Dan
- Department of Orthopedics and Traumatology, Iuliu Hatieganu University of Medicine and Pharmacy, 47 General Traian Mosoiu Street, 400132 Cluj-Napoca, Romania;
| | - Gabriela-Bombonica Dogaru
- Department of Medical Rehabilitation, Iuliu Hatieganu University of Medicine and Pharmacy, 46-50 Viilor Street, 400347 Cluj-Napoca, Romania;
| | - Elena-Mihaela Jianu
- Department of Histology, Iuliu Hatieganu University of Medicine and Pharmacy, 6 Louis Pasteur Street, 400349 Cluj-Napoca, Romania;
| | - Sorin Riga
- Research Center of Physical Chemistry, Department of Chemical Engineering, Faculty of Chemistry and Chemical Engineering, Babes-Bolyai University, 11 Arany Janos Street, 400028 Cluj-Napoca, Romania; (S.R.); (A.M.)
- Academy of Romanian Scientists, 54 Splaiul Independentei, 050085 Bucharest, Romania
| | - Maria Tomoaia-Cotisel
- Research Center of Physical Chemistry, Department of Chemical Engineering, Faculty of Chemistry and Chemical Engineering, Babes-Bolyai University, 11 Arany Janos Street, 400028 Cluj-Napoca, Romania; (S.R.); (A.M.)
- Academy of Romanian Scientists, 54 Splaiul Independentei, 050085 Bucharest, Romania
- Correspondence: (M.T.-C.); (G.T.)
| | - Aurora Mocanu
- Research Center of Physical Chemistry, Department of Chemical Engineering, Faculty of Chemistry and Chemical Engineering, Babes-Bolyai University, 11 Arany Janos Street, 400028 Cluj-Napoca, Romania; (S.R.); (A.M.)
| | - Lucian Barbu-Tudoran
- Electron Microscopy Laboratory Prof. C. Craciun, Faculty of Biology and Geology, Babes-Bolyai University, 5-7 Clinicilor Street, 400006 Cluj-Napoca, Romania;
| | - Gheorghe Tomoaia
- Department of Orthopedics and Traumatology, Iuliu Hatieganu University of Medicine and Pharmacy, 47 General Traian Mosoiu Street, 400132 Cluj-Napoca, Romania;
- Academy of Romanian Scientists, 54 Splaiul Independentei, 050085 Bucharest, Romania
- Correspondence: (M.T.-C.); (G.T.)
| |
Collapse
|